采用熔体旋淬法制备了Ni76Ti5P19和Ni73Ti5Zr3P19 (at%)非晶合金,对其热稳定性及腐蚀行为进行了研究,并讨论了Zr元素的添加对Ni-Ti-P非晶合金性能的影响.结果表明,Zr元素的添加提高了Ni76Ti5P19非晶合金的玻璃转变温度(Tg)和晶化温度(Tx),但使得过冷液体温度区间(△Tx有所降低.电化学实验表明,在NaC1、HC1和H2SO4溶液中,Ni-Ti(-Zr)-P非晶合金发生自钝化,具有良好的耐腐蚀性能,这可能归因于合金表面Ti/Zr和P元素的富集.在同一溶液中,与Ni76Ti5P19非晶合金相比,Ni73Ti5Zr3P19非晶合金具有较高的开路电位和较低的钝化电流密度.在Ni-Ti-P合金中添加元素Zr以替代部分Ni能够在钝化膜中引入ZrO2,从而提高合金表面氧化膜的保护性,改善合金的耐腐蚀能力.
参考文献
[1] | Hashimoto K.;Kim JH.;Yoshioka H.;Mitsui H.;Akiyama E. Habazaki H.;Kawashima A.;Asami K.;Grzesik Z.;Mrowec S.;Park PY. .RECENT PROGRESS IN CORROSION-RESISTANT METASTABLE ALLOYS[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,1995(1/2):1-10. |
[2] | Pang S J;Shek C H;Asami K et al.[J].Journal of Alloys and Compounds,2007,434-435(SI):240. |
[3] | Habazaki H;Ukai H;Izumiya K et al.[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2001,318(1-2):77. |
[4] | Katagiri H;Meguro S;Yamasaki M et al.[J].Corrosion Science,2001,43(01):183. |
[5] | Qin CL;Asami K;Kimura H;Zhang W;Inoue A .Surface characteristics of high corrosion resistant Ni-Nb-Zr-Ti-Ta glassy alloys for nuclear fuel reprocessing applications[J].Electrochemistry communications,2008(9):1408-1410. |
[6] | Zhang T;Pang S J;Asami K et al.[J].Materials Transactions-Japan Institute of Metals,2003,44(11):2322. |
[7] | Pang S J;Shek C H;Zhang T et al.[J].Corrosion Science,2006,48(03):625. |
[8] | Zhang B P;Habazaki H;Kawashima A et al.[J].Corrosion Science,1992,33(05):667. |
[9] | Lee H J;Akiyama E;Habazaki H et al.[J].Corrosion Science,1997,39(02):321. |
[10] | Zhu ZW;Zhang HF;Ding BZ;Hu ZQ .Synthesis and properties of bulk metallic glasses in the ternary Ni-Nb-Zr alloy system[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2008(1/2):221-229. |
[11] | Kawashima A.;Hashimoto K.;Habazaki H. .Highly corrosion-resistant Ni-based bulk amorphous alloys[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2001(0):753-757. |
[12] | Park P Y;Akiyama E;Habazaki H et al.[J].Corrosion Science,1996,38(10):1731. |
[13] | Krolikowski A;Karbownicka B;Jaklewicz O .[J].Electrochimica Acta,2006,51(27):6120. |
[14] | Akatsuka R;Zhang T;Koshiba H et al.[J].Materials Transactions-Japan Institute of Metals,1999,40(03):258. |
[15] | Wolfenden A;Kondlapudi S K R .[J].Journal of Materials Science,1993,28(04):1090. |
[16] | de Boer F R;Boom R;Mattems W C M.Cohesion in Metals[M].Amsterdam:Elsevier Science,1988 |
[17] | Duan G;Xu D;Zhang Q et al.[J].Physical Review,2005,71(22):224208. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%