The main purpose of this study is an in-situ synthesis of (TiB+TiC) hybrid titanium matrix composites (TMCs) by vacuum induction melting method and to verify its mechanical properties. The melting route was adopted to synthesize the commercial pure titanium (cp Ti) and granular boron carbide (B4C). The reinforcements, the fraction of 10 vol. pct, were formed by adding 1.88 wt pct B4C to cp Ti. After in-situ synthesis of TMCs, electron probe micro-analysis elemental mapping was carried out to confirm the distribution and shape of reinforcements. The cone-on-disk type sliding wear test was also done for the identification of TMCs. It is concluded that (TiB+TiC) hybrid TMCs can be in-situ synthesized and has better wear properties than H13.
参考文献
[1] | B Andresen.Die Casting Engineering[M].New York:Marcel Dekker,Inc,2005:289. |
[2] | Z.W.Chen .Formation and progression of die soldering during high pressure die casting[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2005(1/2):356-369. |
[3] | E J Vinarcik.High Integrity Die Casting Process[M].New York:John Wiley and Sons,Inc,2003:101. |
[4] | O Salas;K Kearns;S Carrera;J J Moore .[J].Surface and Coatings Technology,2003,172:117. |
[5] | S C Tjong;Z Y Ma .[J].Material Science and Engineering,2000,29:49. |
[6] | C Leyens;M Peters.Titanium and Titanium Alloys[M].WILEY-VCH,Germany,2003:305. |
[7] | Stanley Abkowitz;Susan M. Abkowitz;Harvey Fisher .CermeTi~R Discontinuously Reinforced Ti-Matrix Composites: Manufacturing, Properties, and Applications[J].JOM,2004(5):37-41. |
[8] | A G Merzhanov .[J].Journal of Materials Chemistry,2004,14:1779. |
[9] | S Ranganath;M Vijayakumar;J Subrahmanyam .[J].Material Science and Engineering,1992,A149:253. |
[10] | C.L. Yeh;S.H. Su .In situ formation of TiAl-TiB_2 composite by SHS[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2006(1/2):150-156. |
[11] | X.Zhang;W.Lu;D.Zhang;R.Wu;Y.Bian;P.Fang .In situtechnique for synthesizing (TiB+TiC)/Ti composites.[J].Scripta materialia,1999(1):39-46. |
[12] | L Christodoulou;D C Nagle;M Brupbacher .[P].US 4751048,1988. |
[13] | D Y Seo;L Zao;J Beddoes .[J].Material Science and Engineering,2002,A329:130. |
[14] | PCPDFWIN version 2.1 Ti:PDF No 44-1294,TiC:PDF No 32-1283,TiB:PDF No 73-2148[Z]. |
[15] | W C Say;Y Y Tsai .[J].Surface and Coatings Technology,2004,176:337. |
[16] | S Y Sung;Y J Kim .[J].Material Science and Engineering,2005,A405:173. |
[17] | S Y Sung;Y J Kim .[P].KO 1020040069535,2006. |
[18] | M W Chase;C A Davies;J R Downey;D J Frurip,R A McDonald A N Syverud.JANAF Thermochemical Table[M].American Chemical Society and American Institute of Physics,United State,1985 |
- 下载量()
- 访问量()
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%