研究了预退火对Sm5Fe74.3Nb1.5Si11.7B4.5C 5 Cu0. 5非晶合金晶化动力学的影响.结果表明,预退火处理使非晶合金晶化相α-Fe和Sm2Fe17Cx的晶化温度(Tp)和晶化表观激活能(Ec)值降低,且改变晶化相a-Fe在晶化过程中晶化激活能的变化趋势,有助于该合金在晶化退火中形成晶粒尺寸较小的α-Fe相.

参考文献

[1] Zhang XY.;Liu JH.;Guan Y.;Zhang JW.;Zhang KQ. .Crystallization kinetics of amorphous Sm8Fe85Si2C5 alloy[J].Journal of Applied Physics,2001(1):496-499.
[2] ZhangX Y;ZhangJW;Wang WK .[J].Journal of Magnetism and Magnetic Materials,2000,219:199-205.
[3] Kuma J.;Kanai Y.;Fukunaga H.;Kitajima N. .Maximum energy product of isotropic Nd-Fe-B-based nanocomposite magnets[J].Journal of Applied Physics,1998(11 Pt.2):6623-6625.
[4] Schrefl T.;Fidler J. .Micromagnetic simulation of magnetizability of nanocomposite Nd-Fe-B magnets[J].Journal of Applied Physics,1998(11 Pt.2):6262-6264.
[5] Schrefl T.;Fidler J. .Modelling of exchange-spring permanent magnets[J].Journal of Magnetism and Magnetic Materials,1998(2):970-975.
[6] 苗卫方;王景唐;李淑苓 .[J].金属学报,1990,26(04):B255-258.
[7] 卢柯;王景唐 .[J].金属学报,1990,26(05):B316-319.
[8] 张湘义;张静武;刘建华 .[J].功能材料与器件学报,1998,4(04):257-259.
[9] Kissinger H E .[J].Analytical Chemistry,1975,29:1702.
[10] 李余增.热分析[M].北京:清华大学出版社,1987:82.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%