对未置氢及置氢Ti-6Al-4V合金进行了TG/DSC试验,研究了置氢钛合金的除氢行为.结果表明,当温度超过600℃时,置氢钛合金的失重规律与未置氢钛合金具有较大的差别.当加热温度在600~900℃之间时,置氢钛合金的失重随着氢含量的增加而增加.这是由于置氢合金中的亚稳相发生了分解.不考虑合金氧化的影响,置氢钛合金的最大失重与合金中的氢含量一致.置氢钛合金的最佳除氢温度为750℃.对于不同氢含量的置氢钛合金,其除氢工艺是相同的.
参考文献
[1] | Yuan, S.J.;Hu, Z.L.;Wang, X.S..Formability and microstructural stability of friction stir welded Al alloy tube during subsequent spinning and post weld heat treatment[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2012:586-591. |
[2] | Zhu, S.;Yang, H.;Guo, L.G.;Gu, R.J..Investigation of deformation degree and initial forming temperature dependences of microstructure in hot ring rolling of TA15 titanium alloy by multi-scale simulations[J].Computational Materials Science,2012:221-229. |
[3] | Yuan, B.G.;Li, C.F.;Yu, H.P.;Sun, D.L. .Influence of hydrogen content on tensile and compressive properties of Ti-6Al-4V alloy at room temperature[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2010(16/17):4185-4190. |
[4] | Chen, Q.;Shu, D.;Zhao, Z. .Microstructure and mechanical properties of AZ91D magnesium alloy prepared by compound extrusion[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2011(10/11):3930-3934. |
[5] | Serre, P.;Figueiredo, R.B.;Gao, N.;Langdon, T.G. .Influence of strain rate on the characteristics of a magnesium alloy processed by high-pressure torsion[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2011(10/11):3601-3608. |
[6] | Chen YX;Wan XJ;Li F;Wang QJ;Liu YY .The behavior of hydrogen in high temperature titanium alloy Ti-60[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2007(1-2):156-159. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%