Under the condition of die casting and reheating temperature of 570-580° C, the Rhe-ological behavior of semi-solid aluminum alloy (A356) is pseudoplasticity at the shearrate of 2×10s-1×104 s-1, and also shows dilatancy at the rate over 106s-1.

参考文献

[1] P A Joly;R Mehrabian .[J].Journal of Materials Science,1976,11(04):1393.
[2] M C Flemings .[J].Metallurgical and Materials Transactions,1991,B22(02):269.
[3] P Kumar;C L Martin;S Brown .[J].Metallurgical and Materials Transactions,1993,A24:1107.
[4] L S Turng;K K Wang .[J].Journal of Materials Science,1991,26(08):2173.
[5] M Hiral;K Takebayashi .[J].ISIJ International,1993,33(02):405.
[6] T Z Kattamas;T J Piccone .[J].Materials Science and Engineering,1991,A131(02):265.
[7] 苏华钦,朱鸣芳,高志强.半固态铸造的现状及发展前景[J].特种铸造及有色合金,1998(05):1-6.
[8] N Wang;G J Shu;H G Yang .[J].Journal of Materials Science,1990,25(08):2185.
[9] K Wang.Heat Transfer,Mix and Flow for the Non-Newtonian Fluid[M].杭州:浙江大学出版社,1988:35.