利用正交设计L25(56)安排实验,分别以矫顽力和磁滞回线的方形度为考察指标,通过极差分析和方差分析优化Co-Pt-W磁性薄膜电沉积制备工艺,结合工业生产的实际需求,得到Na2WO4·2H2O及(NH4)2C6H6O7浓度分别为0.08L、0.198mol/L,电流密度为5mA/cm2,温度为60℃的制备条件为最佳组合.在此条件下制备了Co-Pt-W薄膜样品,并对其磁性能进行验证,对结构和形貌进行了测量.结果表明hcp结构有利于电沉积Co-Pt-W薄膜的硬磁性能.

参考文献

[1] Park D Y;Myung N V;Schwartz M et al.[J].Electrochimica Acta,2002,47:2893-2900.
[2] Ricq L.;Gigandet MP.;Pagetti J.;Lallemand F. .Influence of sodium saccharin on the electrodeposition and characterization of CoFe magnetic film[J].Surface & Coatings Technology,2001(2/3):278-283.
[3] Xun K.;Shen DF. .Grain growth in Co27Pt73 alloy films with perpendicular magnetic anisotropy[J].Journal of Applied Physics,2001(12):8054-8056.
[4] Maranville BB.;Hellman F. .Oxygen-assisted room-temperature deposition of CoPt3 films with perpendicular magnetic anisotropy[J].Applied physics letters,2002(21):4011-4013.
[5] Cavallotti P L;Bestetti M;Franz S .[J].Electrochimica Acta,2003,48:3013-3020.
[6] Zana I;Zangari G;Parkd J W et al.[J].Journal of Magnetism and Magnetic Materials,2004,272-276:e1775-e1776.
[7] 吴琼;葛洪良;卫国英 等.[J].中国稀土学报,2005,23:46-48.
[8] Zana 1;Zangari G .[J].Journal of Magnetism and Magnetic Materials,2004,272:1698-1699.
[9] Rhen F M F;Coey J M D .[J].Journal of Magnetism and Magnetic Materials,2004,272:883-884.
[10] Zana I;Zangari G .[J].Electrochemical and Solid-State Letters,2003,6(12):153-156.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%