Ternary Al-Cu-W alloys were investigated. The previously reported Al(3)Ti-type phase (space group 14/mmm) with the average composition Al(67)Cu(11.5)W(21.5) was found to have a=3.7296(4) angstrom and c=8.3797(10) angstrom. The ternary phase forming around Al(67)Cu(21)W(12) has a hexagonal structure with a=8.6594(13) angstrom and c=15.2677(21) angstrom. (C) 2011 International Centre for Diffraction Data. [DOI: 10.1154/1.3549770]