在真空单辊急冷装置上制取含Cr2-10wt-%的五种Al-Cr合金薄带利用XRD,TEM,电子探针及能谱分析研究了它们的相组成及显微组织,还测定了显微硬度和抗拉强度.实验表明Al-8.0Cr具有较高的显微硬度和最高的强度极限.

Some strips of five Al- (2-10) Wt-% Cr alloys were made on the rapid cooling apparatus with a monoroller.The calculated average cooling rate was about 3-4 x 105℃ / s.The microstructure and the phase consistance of the alloy were studied by XRD, TEM, elect