A novel super-hybrid composite (NSHC) is prepared with three-dimension reticulated SiC ceramic (3DRC), high performance carbon fibers and modified phenolic resin (BPR) in this paper. Ablation performance of super-hybrid composite is studied. The results show that the NSHC has less linear ablation rate compared with pure BPR and CF/BPR composite, for example, its linear ablation rate is 50% of CF/BPR at the same fiber content. Mass ablation rate of the NSHC is slightly lower than that of pure BPR and CF/BPR composite because of their difference in the density. Scanning electron microscopic analysis indicates that 3DRC can increase anti-erosion capacity of materials because its special reticulated structure can control the deformation of materials and strengthen the stability of integral structure.

参考文献

[1] YIDimItrienko .[J].Composites Part A:Applied Science and Manufacturing,1997,28(50):463.
[2] ASahaDeuri;Anil KBhowmick;RGhosh;BJohn,TSriram ,SKDe .[J].Polymer Degradation and Stability,1988,21(01):21.
[3] GSPisarenko;GNTretyachenko .[J].Acta Astronautica,1983,10(07):521.
[4] L.Monney;C.Dubois;A.Chambaudet .Ablation of the organic matrix: fundamental response of a photo-aged epoxy-glass fibre composite[J].Polymer Degradation and Stability,1997(3):357-366.
[5] WeihuiJIANG;Jianer ZHOU;Xingfang HU.[J].Ceramics Technol,2001(04):7.
[6] RRLaher;LRMegill .[J].Planetary and Space Science,1998,36(12):1497.
[7] ZhihaiFENG;Ruilian YU;Chengzhao YAO;Zhongping LI.[J].Aerospace Materials and Technology(in Chinese),2001(06):10.
[8] R. D. Patton;C. U. Pittman Jr.;L. Wang .Ablation, mechanical and thermal conductivity properties of vapor grown carbon fiber/phenolic matrix composites[J].Composites, Part A. Applied science and manufacturing,2002(2):243-251.
[9] PSSreejith;RKrishnamurthy;SKMalhotra;KNarayanasamy .[J].Journal of Materials Processing Technology,2000,104(01):53.
[10] DCho;BIYoom .[J].Composites Science and Technology,2001,61(02):271.
[11] YJLee;HJJoo;Surface .[J].Journal of Coating Technology,2004,180(02):286.
[12] JKPark;DCho;TJKang .[J].CARBON,2004,24:795.
[13] JKPark;TJKang .[J].Carbon,2002,40:2125.
[14] JHenderson;MRTant;GR Moore;JAWiebelt .[J].Thermochimica Acta,1981,44(03):253.
[15] LNHugh;McManus;George SSpringer.[J].Computational Materials Science,1992(26):206.
[16] GuangfuZHANG.[J].Polymer Science and Technology,1990(05):33.
[17] LianshengYAN;Dongmei YAO;Xuejun YANG.[J].宇航材料工艺,2002(02):29.
[18] MohamedOAdalla;ALuduick;TMitchell.[J].POLYMER,2003(40):7353.
[19] JGGao;LXia;YFLiu .[J].Polymer Degradation and Stability,2004,83:71.
[20] ZhihaiFENG;Ruilian YU;Chengzhao YAO;Zhongping LI.[J].Aerospace Materials and Technology(in Chinese),2001(06):10.
[21] GYTang;YJYan;XNChen.[J].Materials & Design,2001(22):21.