生物活性材料是生物医用材料领域中一个重要的研究方向.研究表明,在体液的作用下这类材料的表面能够形成Si-OH、Ti-OH、Ta-OH、-COOH和PO4H2等功能基团,从而诱导类骨磷灰石层生成并与骨发生键合.综述了人们利用医用金属进行表面生物活化或通过有机/无机复合的方法得到力学性能良好的新型生物活性材料,为人工植入体的临床应用提供了更广阔的前景.
参考文献
[1] | Wang M .Developing bioactive composite materials for tissue replacement.[J].Biomaterials,2003(13):2133-2151. |
[2] | Kim Cheol Y;Jee Sang Soo .Hydroxyapatite formation on bioactive-glazed alumina[J].Journal of the European Ceramic Society,2003,23(11):1803. |
[3] | Borrajo J P;Gonz AAlez P;Liste S .The role of the thickness and the substrate on the in vitro bioactivity of silicabased glass coatings[J].Materials Science and Engineering C,2005,25:187. |
[4] | Verné E;Fernández Vallés C;Vitale Brovarone C et al.Double-layer glass-ceramic coatings on Ti6Al4V for dental implants[J].Journal of the European Ceramic Society,2004,24(09):2699. |
[5] | Rich Jaana;Jaakkola Tiina;Tirri Teemu et al.In vitro evaluation of poly-caprolactone-co-DL-lactide/bioactive glass composites[J].Biomaterials,2002,23(10):2143. |
[6] | Peitl O;Oréfice R L;Hench L L et al.Effect of the crystallization of bioactive glass reinforcing agents on the mechanical properties of polymer composites[J].Materials Science and Engineering A,2004,372:245. |
[7] | Blaker JJ;Nazhat SN;Boccaccini AR .Development and characterisation of silver-doped bioactive glass-coated sutures for tissue engineering and wound healing applications.[J].Biomaterials,2004(7/8):1319-1329. |
[8] | Neo M;Nakamura T;Ohtsuki C et al.Apatite formation on three kinds of bioactive materials at an early stage in vivo:a comparative study by transmission electron microscopy[J].Journal of Biomedical Materials Research,1993,27:999. |
[9] | kokubo T;Kushitani H;Sakka S et al.Solutions able to reproduce in vivo surface-structure changes in bioactive glass-ceramic A-W3[J].Journal of Biomedical Materials Research,1990,24:721. |
[10] | Kim H M;Miyaji F;Kokubo T et al.Bioactivity of M2OTiO2-SiO2 M=Na,K glasses:an in vitro evaluation[J].Bulletin of the Chemical Society of Japan,1996,69:2387. |
[11] | Wei M;Uchida M;Kim HM;Kokubo T;Nakamura T .Apatite-forming ability of CaO-containing titania.[J].Biomaterials,2002(1):167-172. |
[12] | UCHIDA M;Kim H M;Kokubo T et al.Structural dependence of apatite formation on zirconia gel in simulated body fluid[J].Journal of the Ceramic Society of Japan,2002,110:710. |
[13] | Tanakama K;Kim H M;Kokubo T et al.Mechanism of biomineralization of apatite on a sodium silicate glass:TEMEDX study in vitro[J].CHEMISTRY OF MATERIALS,2001,13:1108. |
[14] | Tanakama K;Kim H M;Kokubo T et al.X-ray photoelectron on a sodium silicate glass in simulated body fluid[J].Journal of the American Ceramic Society,2002,85:1933. |
[15] | UCHIDA M;Kim H M;Kokubo T.Biceramic[M].World Sci Singapore,1999:149. |
[16] | Tadashi Kokubo;Hyun-Min Kim;Masakazu Kwashita .Novel bioactive materials with different mechanical properties[J].BIOMATERIALS,2003,24:2162. |
[17] | Niwa J .Acceleration of bone-repair using hudroxyapatite[J].Bone Fracture,1983,5:124. |
[18] | Himeno T;Kawashita M;Kim H M.Zeta-potential variation of bioactive titanium metal during apatite formation on its surface in simulated body fluid[A].Switzerland.Trans Tech Pubilshers,2001:641. |
[19] | Kitahara F;Furusawa K;Ozaki T.Zeta potential[M].Tokyo.Saientisuto-sha,1997 |
[20] | Kim HM;Takadama H;Kokubo T;Nishiguchi S;Nakamura T .Formation of a bioactive graded surface structure on Ti-15Mo-5Zr-3Al alloy by chemical treatment.[J].Biomaterials,2000(4):353-358. |
[21] | Kim H M;Miyaji F;Kokubo T et al.Bonding strength of bonelike apatite layer to Ti metal substrate[J].Journal of Biomedical Materials Research Part B:Applied Biomaterials,1997,38:121. |
[22] | Kim H M;Sasaki Y;Suzuki J.Mechanical properties of bioactive titanium prepared by chemical treatment[A].Switzerland.Trans Tech Publishers,2000:227. |
[23] | Nishiguchi S;Kato H;Neo M et al.Alkaliand heat-treated porous titanium for orthopedic implants[J].Journal of Biomedical Materials Research,2001,54:198. |
[24] | Miyazaki T;Kim H M;Kokubo T et al.Enhancement of bonding strength by graded structure at interface between apatite layer and bioactive tantalum metal[J].Journal of Materials Science:Materials in Medicine,2002,13:651. |
[25] | 俞耀庭;张兴栋.生物医用材料[M].天津:天津大学出版社,2000:116. |
[26] | Kawashita M;Nakao M;Minoda M;Kim HM;Beppu T;Miyamoto T;Kokubo T;Nakamura T .Apatite-forming ability of carboxyl group-containing polymer gels in a simulated body fluid.[J].Biomaterials,2003(14):2477-2484. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%