通过简单水热法成功制备了Co3O4纳米材料.利用常见配合物Co(NH3)6Cl3在水热条件下具有解离倾向,通过控制其浓度得到不同尺寸的Co3O4纳米颗粒.实验表明,此类反应中配离子解离占主导作用,表面活性剂的添加量对产物形貌的影响不明显,而反应物浓度对产物形貌和尺寸的影响较大,随着反应物Co(NH3)6Cl3浓度的增加,产物尺寸先增大后减小.并且推测了不同尺寸纳米颗粒可能的形成机理.
参考文献
[1] | Jiang Y.;Wu Y.;Xie B.;Xie Y.;Qian YT. .Moderate temperature synthesis of nanocrystalline Co3O4 via gel hydrothermal oxidation[J].Materials Chemistry and Physics,2002(2):234-237. |
[2] | Li WY;Xu LN;Chen J .Co3O4 nanomaterials in lithium-ion batteries and gas sensors[J].Advanced functional materials,2005(5):851-857. |
[3] | Feng J.;Zeng HC. .Size-controlled growth of Co3O4 nanocubes[J].Chemistry of Materials,2003(14):2829-2835. |
[4] | Youngjo Tak;Kijung Yong .A Novel Heterostructure of Co3O4/ZnO Nanowire Array Fabricated by Photochemical Coating Method[J].The journal of physical chemistry, C. Nanomaterials and interfaces,2008(1):74-79. |
[5] | Mohandes, F;Davar, F;Salavati-Niasari, M .Preparation of Co3O4 nanoparticles by nonhydrolytic thermolysis of [Co(Pht)(H2O)](n) polymers[J].Journal of Magnetism and Magnetic Materials,2010(7):872-877. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%