采用二次阳极氧化工艺制备了高度有序的多孔氧化铝模板,通过模板法与溶胶.电泳沉积法结合的组装技术,合成了具有高比表面积的糖葫芦状M/TiO2(M=La3+,Fe3+)纳米线阵列体系.采用SEM对样品进行了表征,测试结果表明:Ti02纳米线阵列保持了模板的有序性,直径分布均匀一致,为70 nm左右,长为15μm左右,取向性很好.以甲基橙为目标降解物,在可见光下考察该金属离子掺杂纳米线的催化活性,结果显示此纳米线阵列体系具有非常优良的可见光催化性能,与同条件下制备的薄膜试样相比可见光催化活性可以提高4倍以上.
参考文献
[1] | Wang R;Hashimoto K;Fujishima A et al.[J].Nature,1997,388:431. |
[2] | Masakazu A;Masato T .[J].Journal of Catat,2003,216:505. |
[3] | Ara(n)la J;Do(n)a-Rodriguez J M;Herrera Melifin J A et al.[J].Journal of Photochemistry and Photobiology A:Chemistry,2005,174(01):7. |
[4] | Choi W;Terrain A;Hoffmann M R T .[J].Journal of Physical Chemistry,1994,98(51):13669. |
[5] | Srinivasan S S;Wade J;Stefanakos E K.[J].Journal of Alloys and Compounds,2006(424):322. |
[6] | Alexej M;Diyya A;Cheng G S et al.[J].Chemical Physics Letters,2001,349:1. |
[7] | Steven J L;Seans S;Yun W et al.[J].Advanced Functional Materials,2002,12(01):59. |
[8] | Arana J;Gonz(a)lez Diaz O;Miranda Saracho M .[J].Applied Catalysis B:Environmental,2001,32(1-2):49. |
[9] | LIU Xiang-zhi,XU Ming-xia,TIAN Yu-ming,SHANG Meng,ZHANG Ping.Regularity control of porous anodic alumina and photodegradation activity of highly ordered titania nanostructures[J].中国有色金属学会会刊(英文版),2006(z1):341-344. |
[10] | 田玉明,徐明霞,刘祥志,戈磊,张平.糖葫芦状二氧化钛纳米线阵列的制备及其光催化性能[J].催化学报,2006(08):703-707. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%