以六水合硝酸钴和酞酸丁酯为主要原料,乙二胺四乙酸(EDTA)为络合剂,用溶胶-凝胶法制备出CoTiO3纳米晶.用差热-失重热分析(TG-DSC)、X-射线衍射(XRD)、透射电子显微镜(TEM)等测试手段,对凝胶前驱体及产物进行了表征.研究了煅烧温度、前驱体pH值对产物组成和结构形貌的影响,并用Kissinger法计算CoTiO3纳米晶的表观活化能.结果表明:溶胶pH值为2.0~4.0,凝胶经700℃煅烧2h,获得均匀分布的CoTiO3纳米晶、平均粒径约50 nm.CoTiO3纳米晶的表观活化能为80.43 kJ/mol.
参考文献
[1] | Zhou L;Zhang SY;Cheng JC;Zhang LD;Zeng Z;NANJING UNIV LAB MODERN ACOUST NANJING 210093 PEOPLES R CHINA.;ACAD SINICA INST SOLID STATE PHYS HEFEI 230031 PEOPLES R CHINA. .Optical absorptions of nanoscaled CoTiO3 and NiTiO3[J].Materials Science & Engineering, B. Solid-State Materials for Advanced Technology,1997(2):117-122. |
[2] | 高文元,孙俊才.机械力化学合成CoTiO3纳米晶的研究[J].功能材料,2004(06):766-768. |
[3] | Sharma, YK;Kharkwal, M;Uma, S;Nagarajan, R .Synthesis and characterization of titanates of the formula MTiO3 (M = Mn, Fe, Co, Ni and Cd) by co-precipitation of mixed metal oxalates[J].Polyhedron,2009(3):579-585. |
[4] | 周国伟,陈代荣,徐桂英.钛铁矿型CoTiO3纳米材料的制备及性能表征[J].化学学报,2005(20):1917-1920. |
[5] | Siemons M;Simon U .Gas sensing properties of volume-doped CoTiO3 synthesized via polyol method[J].Sensors and Actuators, B. Chemical,2007(2):595-603. |
[6] | Lin YJ;Chang YH;Yang WD;Tsai BS .Synthesis and characterization of ilmenite NiTiO3 and CoTiO3 prepared by a modified Pechini method[J].Journal of Non-Crystalline Solids: A Journal Devoted to Oxide, Halide, Chalcogenide and Metallic Glasses, Amorphous Semiconductors, Non-Crystalline Films, Glass-Ceramics and Glassy Composites,2006(8):789-794. |
[7] | M. Enhessari;A. Parviz;K. Ozaee;E. Karamali .Magnetic properties and heat capacity of CoTiO_3 nanopowders prepared by stearic acid gel method[J].Journal of Experimental Nanoscience,2010(1/2):61-68. |
[8] | 彭秧锡,雷芳.凝胶燃烧法制备纳米CoTiO3粉体及其表征[J].人工晶体学报,2008(06):1551-1554. |
[9] | 肖宗湖,ZHANG Meng,郭米艳.溶胶-凝胶法制备ZnO薄膜的特性研究[J].人工晶体学报,2008(04):1003-1007. |
[10] | 郝品,黄剑锋,曹丽云,吴建鹏,贺海燕.NiTiO3纳米晶的溶胶-凝胶制备工艺研究[J].人工晶体学报,2010(02):336-340. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%