应用扫描电镜分析、能谱分析和显微镜技术等分析手段,研究了结晶器电磁搅拌对IF钢铸坯表层纯净度的影响。结果表明:结晶器电磁搅拌可有效改善铸坯表面质量,使铸坯表层皮下气泡和显微夹杂物显著减少;IF钢铸坯中夹杂物主要是Al2O3、TiN和Al2O2TiN、Al2O3-Ti2O2、Al2O3-Ti2O3-TiN型复合夹杂物;铸坯表层皮下气孔在铸坯宽度和厚度方向上均呈非均匀分布,气泡直径主要分布在50-350μm之间。

Effects of M-EMS on surface cleaniness of IF steel slab were investigated by means of SEM, EDS and microscopic techniques, etc. The results indicate that M-EMS can improve surface cleanliness and reduce inclusions, blow hole defects effectively. Al2 03 , TiN and Al2 O3-TiN, Al2 03 Ti2 O3 , A12 O3-Ti2 O3-TiN are main inclusions in the slab. The distribution of bubbles in slabs is non-homogeneous in respect of width and depth, the bubble size range of 50 to 350μm.

参考文献

[1] 马衍伟,王先进.超深冲IF钢研究的最新进展[J].钢铁,1998(04):0.
[2] Hiroshi Takechi .The Development of Interstitial Free Steel in Japan[J].ISIJ International,1994,34(01):1.
[3] Emling W H;Waugaman T A.Subsurface Mold Slag Entrainment in Ultra Low Carbon Steels[A].Warrendale:ISS-AIME,1994:371.
[4] Kimura H.Advances in High-Purity IF Steel Manufacturing Technology[J].NIPPON STEEL TECHNICAL REPORT,1994(61):65.
[5] Inoue T;Yamanaka R;Yasunaka H.Mechanism of Sliver Defect Formation in Ultra Low-Carbon Steels[A].Montreal:Canad Inst Min,Metallurgy and Petroleum,1994:325.
[6] Ohtani Y;Fukuda J;Ishiwata N.Improvement of Surface Quality With In-Mold Electromagnetic Stirring[J].Current Advances in Materials and Processes,1994(07):1194.
[7] Okano S;Nishimura T;Ohi H.Relation Between Large Inclusions and Growth Directions of Columnar Dendrites in Continuously Cast Slabs[J].Tesu-to-Hagane,1975(61):2982.
[8] Dijk J;Manneveld D;Rabenberg J M.In Plant Assessment of Steel Cleanliness in Continuously Cast Slabs and Hot Rolled Coils[J].Ironmaking and Steelmaking,1993(20):75.
[9] Nakashima J;Fukuda J;Kiyose A.Improvement of Transition Part of Slab Surface Cleanliness With In Mold Electromagnetic Stirring[J].Tesu-to Hagane,2007(93):281.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%