发现正交结构的高压相β-TiO2可通过高能球磨锐钛矿TiO2而得到.高能机械球磨减小了颗粒尺寸,球磨40h后,发现样品存在2nm~4nm的类点状颗粒和10nm~35nm的类花瓣状颗粒.高能球磨改变了锐钛矿TiO2晶粒的晶格常数.该晶格畸变现象可能与晶界区行为相关.红外吸收峰随球磨而先"蓝移"后"红移".该"蓝移"与"红移"与晶格常数a的变化紧密相关.另外发现随着球磨时间增长,TiO2的光催化效果变差.
参考文献
[1] | Sukharev V;Wold A;Gao Y M et al.Photoassisted Decomposition of Salicylic Acid on TiO2 and Pd/TiO2 Film[J].Journal of Solid State Chemistry,1995,119:339. |
[2] | Birkefeld L D;Azad A M;Akbar S A .Carbon Monoxide and Hydrogen Detection by Anatase Modification of Titanium Dioxide[J].Journal of the American Ceramic Society,1992,75:2964. |
[3] | Pouilleau J.;Groult H.;Marcus P.;Devilliers D. .SURFACE STUDY OF A TITANIUM-BASED CERAMIC ELECTRODE MATERIAL BY X-RAY PHOTOELECTRON SPECTROSCOPY[J].Journal of Materials Science,1997(21):5645-5651. |
[4] | Hoffmann M R;Martin S T;Choi W et al.Environmental Application of Semiconductor Photocatalysis[J].Chemical Reviews,1995,95:69. |
[5] | Shen TD.;Wang KY.;Quan MX.;Wang JT.;Koch CC. .SOLID-STATE REACTION IN NANOCRYSTALLINE FE/SIC COMPOSITES PREPARED BY MECHANICAL ALLOYING[J].Journal of Materials Science,1997(14):3835-3839. |
[6] | Cho Y S;Koch C C .Amorphization by Mechanical Attrition in the Nb- Ge System:Extension of the Amorphous Composition Range[J].Materials Science and Engineering A,1993,161:65. |
[7] | Jia D C;Zhou Y;Lei T C .Microstructure and Mechanical Properties of Al- 12Ti- 6Nb Prepared by Mechanical Alloying[J].Materials Science and Engineering A,1997,232:183. |
[8] | 刘新宽,马明亮,席生歧,周敬恩,王渠东,丁文江.机械力活化合成机制研究[J].稀有金属材料与工程,2000(06):382-385. |