Poly(para-xylylene) hollow fibers with inner diameters can be prepared via template fibers electrospun from solutions.The PPX is deposited from the vapor phase and the template fiber is selectively removed by heat treatment or solvent extraction. The PPX is partially crystalline and the crystal modification depending on the route is used to extract the template fiber. The thermal stability of the hollow fibers is only slightly reduced relative to the bulk material and the same holds for the UV-stability.

参考文献

[1] GMWhitesides;JPMathias;CTSeto .[J].科学(上海),1991,254:1312.
[2] GAOzin .[J].Advanced Materials,1992,4:612.
[3] JMSchnur .[J].Science,1993,262:166.
[4] CRMartin .[J].Science,1994,266:1961.
[5] FTEdelmann .[J].Angewandte Chemie,1999,11:1473.
[6] FTEdelmann .[J].Angewandte Chemie International Edition,1999,38:1381.
[7] SIjima .[J].Nature,1991,354:56.
[8] MGhadiri;JRGranja;LBuehler .[J].Nature,1994,369:301.
[9] CRMartin .[J].Accounts of Chemical Research,1995,28:61.
[10] EEvans;HBrownman;ALeung;DNeedham , DTirrell .[J].Science,1996,273:933.
[11] RAdert;TLiu;JHWendorff .[J].Journal of Polymer Science Part A:Polymer Chemistry,2003,41:545.
[12] Mognitzki;WCzado;TFrese;ASchaper, MHellwig, MSteinhart, AGreiner , JHWendorff .[J].Advanced Materials,2001,13:70.
[13] PKaumgarten .[J].Journal of Colloid and Interface Science,1971,36:71.
[14] JLarr o;RSJManley .[J].Journal of Polymer Science Part B:Polymer Physics,1981,19:909.
[15] JLarr o;RSJManley .[J].Journal of Polymer Science Part B:Polymer Physics,1981,19:921.
[16] JLarr o;RSJManley .[J].Journal of Polymer Science Part B:Polymer Physics,1981,19:933.
[17] JNDoshi;GShrinivasan;DHReneker .[J].Polymer News,1995,20:206.
[18] JNDoshi;GShrinivasan;DHReneker .[J].Journal of Electrostatics,1995,35:151.
[19] XTang;DHReneker .[J].Journal of Macromolecular Sciences:Physics,1997,36:169.
[20] DHReneker;IChun .[J].NANOTECHNOLOGY,1996,7:216.
[21] RJaeger;HSchonherr;GJVansco .[J].Macromolecules,1996,29:7634.
[22] RJaeger;MMBerghof;CMBattle;HSchonherr ,GJVansco .[J].Macromolecular Symposia,1981,127:141.
[23] HFong;DHReneker .[J].Journal of Polymer Science Part B:Polymer Physics,1999,37:3488.
[24] DHReneker;ALYarin;HFong;SKoombhongse .[J].Journal of Applied Physics,2000,87:9.
[25] ALYarin;SKoombhongse;DHReneker .[J].Journal of Applied Physics,2001,89:3018.
[26] WFGorham.[J].Journal of Polymer Science Part A:Polymer Chemistry,1966(04):3027.
[27] CSchmidt;VStiimpflen;JHWendorff;AHasenhindl, WGronski, MIshaque , AGreine .[J].ACTA POLYMERICA,1998,49:232.
[28] Mera;ARivaton;CG,on;JLGardette .[J].European Polymer Journal,2000,36:1753.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%