采用烧结法,选用Na2O-B2O3-SiO2为基础玻璃(NBS),按照氟磷灰石组成配比添加CaO,P2O5,CaF2三种组分,制备Na2O-B2O3-SiO2-CaO-P2O5-CaF2生物微晶玻璃.利用差热分析、X射线衍射分析及扫描电镜等测试手段对微晶玻璃物相、微观结构进行了测试和分析,并采用模拟体液对样品的生物活性进行了验证.结果表明:随着热处理温度升高,样品的晶化程度逐步提高,当热处理温度在750℃时,可以获得主晶相为氟磷灰石,晶粒尺寸在100 nm左右、其晶化率≥80%的微晶玻璃样品,通过模拟体液浸泡实验证明了样品具有一定的生物活性.

参考文献

[1] H.C. Li;D.G. Wang;J.H. Hu;C.Z. Chen.Effect of the partial substitution of K_2O, MgO, B_2O_3 for CaO on crystallization, structure and properties of Na_2O-CaO-SiO_2-P_2O_5 system glass-ceramics[J].Materials Letters,2013Sep.1(Sep.1):373-376.
[2] Kai Huang;Shu Cai;Guohua Xu.Preparation and characterization of mesoporous 45S5 bioactive glass-ceramic coatings on magnesium alloy for corrosion protection[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2013:290-297.
[3] Karem Noris-Suarez;Maritza Vasquez;Yotselys Lopez.Osteoblastic cells biomineralized on bioactive glass and glass-ceramics of the SiO2.Na2O.CaO.K2O.MgO.P2O5 system modified with Al2O3 and B2O3[J].Journal of Ceramic Processing Research. (Text in English),20102(2):129-137.
[4] 王玥;田清波;岳雪涛;王修慧;高宏.CaO-MgO-Al2O3-SiO2-P2O5-(F)微晶玻璃的析晶及特征[J].人工晶体学报,2007(3):692-695.
[5] Tae Wan Kim;Su Chak Ryu;Byung Kyu Kirn.Porous Hydroxyapatite Scaffolds Containing Calcium Phosphate Glass-Ceramics Processed Using a Freeze/Gel-Casting Technique[J].Metals and Materials International,20141(1):135-140.
[6] 丁国军;余献忠;杨贤燕;陈晓怡;王冶根;骆旭康;苟中入.溶胶-凝胶低熔点硼硅酸盐生物活性玻璃增强高温熔融45S5生物玻璃多孔材料[J].材料科学与工程学报,2013(6):852-858.
[7] 方一航;王焕平;李志刚;黄小华;赵先锐;李勤涛.Bi2O3助熔剂对CaO-B2O3-SiO2/Al2O3玻璃-陶瓷复合材料性能的影响[J].复合材料学报,2014(6):1509-1515.
[8] 单小宏;刘咏.定向排列玻璃陶瓷的研究进展[J].粉末冶金材料科学与工程,2004(3):238-242.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%