硅橡胶凭借其诸多优异性能在国防与民用领域获得了越来越广泛的应用,成为其他材料所不能相比和替代的高分子材料,但力学性能差严重制约其发展,因此硅橡胶改性一直是科技工作者关注的焦点.重点从化学改性、添加功能填料两个方面阐述了国外在硅橡胶改性方面的研究进展,并综述了近几年国外在硅橡胶材料性能评估方面开展的研究工作,提出硅橡胶材料未来的发展方向.
参考文献
[1] | 谢尊虎,曾凡伟,肖建斌.硅橡胶性能及其研究进展[J].特种橡胶制品,2011(02):69-72. |
[2] | 涂婷,陈福林,岑兰,周彦豪.硅橡胶的物理改性研究进展[J].弹性体,2010(02):77-82. |
[3] | SkanderMani;PhilippeCassagnau;MostoBousmina;PhilippeChaumont .Cross-LinkingControlofPDMSRubberatHighTemperaturesUsingTEMPONitroxide[J].Macromolecules,2009(21):8460-8467. |
[4] | Radhashyam Giri;Kinsuk Naskar;Golok Behari Nando .Insite compatibilization of linear low-density polyethylene (LLDPE) and polydimethyl siloxane (PDMS) rubber through reactive blending[J].Mater Express,2012,2(01):37. |
[5] | Muhammad Imran Malik;Pritish Dinha et al.Characterization of polydimethylsiloxane-block-polystyrene copolymers by liquid chromatography at critical conditions[J].Macromolecular Chemistry and Physics,2011,212:1221. |
[6] | Johan G Alauzun et al.Biocompatible,hyaluronic acid modified silicone elastomers[J].BIOMATERIALS,2010,31:3471. |
[7] | 王林,张利,刘小兰,李金辉.硅橡胶补强填料的研究进展[J].山东化工,2010(12):33-36. |
[8] | Cohen-Addad J P;Roby C;Sauviat M .Characterization of chain binding to filler in silicone-silica systems[J].POLYMER,1985,26:1231. |
[9] | Capel-Sanchez M C et al.Silylation and surface properties of chemically grafted hydrophobic silica[J].Journal of Colloid and Interface Science,2004,277:146. |
[10] | Zhou Hua;Wang Hongxia et al.Fluoroalkyl silane modified silicone rubber/nanoparticle composite:A super durable,robust superhydrophobic fabric coating[J].Advanced Materials,2012,24:2409. |
[11] | Mora-Barrantes I;Rodriguez A et al.Overcoming the disadvantages of fumed silica as filler in elastomer composites[J].Journal of Materials Chemistry,2011,21:7381. |
[12] | Silva V P;Paschoali M P;Goncalves M C et al.Silicone rubbers filled with TiO2:Characterization and photocatalytic activity[J].Materials Chemistry and Physics,2009,113(01):395. |
[13] | Iqbal, N.;Khan, M.B.;Sagar, S.;Maqsood, A. .Fabrication and characterization of multiwalled carbon nanotubes/silicone rubber composites[J].Journal of Applied Polymer Science,2013(4):2439-2446. |
[14] | Raquel Verdejo et al.Physical properties of silicone foams filled with carbon nanotubes and functionalized grapheme sheets[J].European Polymer Journal,2008,44:2790. |
[15] | Theodore F et al.Synthesis and characterization of novel PDMS nano-composites using POSS derivatives as crosslinking filler[J].J Polym Chem,2009,47:2589. |
[16] | James P Lewicki et al.Effect of meta-Carborane on segmental dynamics in a bimodal poly(dimethylsiloxane) network[J].MACROMOLECULES,2008,41:9179. |
[17] | Anca Serbescu;Kay Saalwachter .Particle-induced network formation in linear PDMS filled with silica[J].POLYMER,2009,50:5434. |
[18] | Timothy Ratti et al.Polymer filler aging and failure studied by lateral force microscopy[R].LLNL-TR-413497,2009. |
[19] | Stickney P B;Falb R D .Carbon black-rubber interactions and bound rubber[J].Rubber Chem Techn,1964,37:1299. |
[20] | Mirta I Aranguren et al.Compounding fumed silicas into polydimethylsiloxane:Bound rubber and final aggregate size[J].Journal of Colloid and Interface Science,1997,195:329. |
[21] | Nakamae K;Matsui J et al.New analytical methods for the surface/interface and the micro-structures in advanced nanocomposite materials by synchrotron radiation[J].Atom Indonesia,2010,36(03):125. |
[22] | Kueseng K;Jacob KI .Natural rubber nanocomposites with SiC nanoparticles and carbon nanotubes[J].European Polymer Journal,2006(1):220-227. |
[23] | Lee Seung-woo;Sigmund Wolfgang M .AFM study of repulsive van der Waals forces between Teflon AFTM thin film and silica or alumina[J].Colloids and Surfaces,2002,204:43. |
[24] | Julie L Herberg et al.Characterization of local deformation in filled-silicone elastomers subject to high strain-NMR MOUSE and magnetic resonance imaging as a diagnostic tool for detection of inhomogenetities[J].Polymer Degradation and Stability,2006,91(08):1701. |
[25] | David E.Hanson;Marilyn Hawley;Robert Houlton;Kiran Chitanvis;Philip Rae .Stress softening experiments in silica-filled polydimethylsiloxane provide insight into a mechanism for the Mullins effect[J].Polymer: The International Journal for the Science and Technology of Polymers,2005(24):10989-10995. |
[26] | Mogon Patel;Paul Morrell et al.Compexities associated with moisture in foamed polysiloxane composites[J].Polymer Degradation and Stability,2008,93:513. |
[27] | Robert S Maxwell et al.Quantification of radiation induced crosslinking in a commercial,toughened silicone rubber,TR55 by 1H MQ-NMR[J].Polymer Degradation and Stability,2009,94:456. |
[28] | Mogon Pate et al.Compression set in gas-blown condensation cured polysiloxane elastomers[J].Polymer Degradation and Stability,2010,95:2499. |
[29] | Sarah Chinn et al.Chemical origins of permanent set in a peroxide cured filled silicone elastomer-tensile and 1H NMR analysis[J].Polymer Degradation and Stability,2006,91:555. |
[30] | Fernando, M.A.R.M.;Gubanski, S.M. .Ageing of silicone rubber insulators in coastal and inland tropical environment[J].IEEE transactions on dielectrics and electrical insulation: A publication of the IEEE Dielectrics and Electrical Insulation Society,2010(2):326-333. |
[31] | Tong Cui;C.-W. Lin;C.H. Chien;Y.J. Chao;J.W. Van Zee .Service life estimation of liquid silicone rubber seals in polymer electrolyte membrane fuel cell environment[J].Journal of Power Sources,2011(3):1216-1221. |
[32] | Arianpour F et al.Hydrophobic and ice-retarding properties of doped silicone rubber coatings[J].Applied Surface Sinence,2013,265:546. |
[33] | Leland M Vane et al.Factors affecting alcohol-water perva poration performance of hydrophobic zeolite-silicone rubber mixed matrix membranes[J].Journal of Membrane Science,2010,364(1-2):102. |
[34] | Kim, E.S.;Kim, E.J.;Lee, T.H.;Yoon, J.S. .Improvement of the adhesion properties of silicone rubber by the incorporation of silane-modified montmorillonite[J].Journal of Applied Polymer Science,2013(4):2563-2570. |
[35] | Kashani M Razzaghi;Javadi S;Gharavi N .Dielectric properties of silicone rubber-titanium dioxide composites prepared by dielectrophoretic assemble of filler particles[J].Smart Materials and Structures,2010,19:035019. |