以TiCl3为前驱物,在前驱物中添加一定的钛酸钠纳米管,在水热条件下,合成了锐钛矿相TiO2纳米晶体.其工艺参数为:1.0 mol/L KF为矿化剂,填充度为68%,150 ℃恒温保持24 h.生成的晶体形貌为块状.当添加经400 ℃烧结过的钛酸纳米管时,合成了棒状锐钛矿晶体,晶体直径约为10 nm,长度约为30~100 nm,最大长径比约为5:1.研究了在前驱物中添加不同的纳米管时对生成物的影响.

参考文献

[1] Kakiuchi K;Hosono E;Imai H;Kimura T;Fujihara S .{111}-faceting of low-temperature processed rutile TiO2 rods[J].Journal of Crystal Growth,2006(2):541-545.
[2] Jiang BP;Yin HB;Jiang TS;Jiang YH;Feng H;Chen KM;Zhou WP;Wada YJ .Hydrothermal synthesis of rutile TiO2 nanoparticles using hydroxyl and carboxyl group-containing organics as modifiers[J].Materials Chemistry and Physics,2006(2/3):231-235.
[3] 郑燕青,施尔畏,李汶军,陈之战,仲维卓,胡行方.水热条件下二氧化钛晶体同质变体的形成[J].中国科学E辑,2001(03):204-212.
[4] 郑燕青,施尔畏,元如林,李汶军,王步国,仲维卓,胡行方.二氧化钛晶粒的水热制备及其形成机理研究[J].中国科学(E辑),1999(03):206-213.
[5] Cho CH;Han MH;Kim DH;Kim DK .Morphology evolution of anatase TiO2 nanocrystals under a hydrothermal condition (pH=9.5) and their ultra-high photo-catalytic activity[J].Materials Chemistry and Physics,2005(1):104-111.
[6] Yang J;Mei S;Ferreira JMF;Norby P;Quaresma S .Fabrication of rutile rod-like particle by hydrothermal method: an insight into HNO3 peptization[J].Journal of Colloid and Interface Science,2005(1):102-106.
[7] Pavasupree S;Ngamsinlapasathian S;Suzuki Y et al.Preparation and Characterization of High Surface Area Nanosheet Titania with Mesoporous Structure[J].Materials Letters,2007,61(14-15):2973-2977.
[8] 王芹,陶杰,翁履谦,徐国跃,王秀华,王函.氧化钛纳米管的水热法合成机理研究[J].南京航空航天大学学报,2005(01):130-134.
[9] Nian J;Teng H .Hydrothermal Synthesis of Single-crystalline Anatase TiO2 Nanorods with Nanotubes as the Precursor[J].Journal of Physical Chemistry B,2006,110(09):4193-4198.
[10] Yu HG;Yu JG;Cheng B;Zhou MH .Effects of hydrothermal post-treatment on microstructures and morphology of titanate nanoribbons[J].International Journal of Quantum Chemistry,2006(2):349-354.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%