Ti2AlC and Ti3AlC2 are the most light-weight and oxidation resistant layered ternary carbides belonging to the MAX phases. This review highlights recent achievements on the processing, microstructure, physical, mechanical and chemical properties of these two machinable and electrically conductive carbides. Ti2AlC and Ti3AlC2 display superior properties such as fracture toughness, electrical and thermal conductivities, and oxidation resistance over their binary counterpart. This paper provides a comprehensive overview of the processing-microstructure-property correlations of these two carbides. Potential fields of applications for Ti2AlC and Ti3AlC2 are surveyed. In addition, we point out methods for further improving their properties in some specific applications through appropriate structural design and modification.

参考文献

[1] X. H. Wang;Y. C. Zhou .Microstructure and properties of Ti_3AlC_2 prepared by the solid-liquid reaction synthesis and simultaneous in-situ hot pressing process[J].Acta materialia,2002(12):3141-3149.
[2] N.V.Tzenov;M.W.Barsoum .Synthesis and characterization of Ti_3AlC_2[J].Journal of the American Ceramic Society,2000(4):825-832.
[3] W.B. Zhou;B.C. Mei;J.Q. Zhu;X.L. Hong .Rapid synthesis of Ti_2AlC by spark plasma sintering technique[J].Materials Letters,2005(1):131-134.
[4] C.L.Yeh;Y.G. Shen .Combustion synthesis of Ti_3 A1C_2 from Ti/Al/C/TiC powder compacts[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2008(1/2):308-313.
[5] C.L. Yeh;Y.G. Shen .Effects of TiC and Al_4C_3 addition on combustion synthesis of Ti_2AlC[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2009(1/2):424-428.
[6] C.L. Yeh;Y.G. Shen .Effects of using Al_4C_3 as a reactant on formation of Ti_3AlC_2 by combustion synthesis in SHS mode[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2009(1/2):408-413.
[7] C.J. Lee;J.I. Chae .Effect of #beta#-Si_3N_4 starting powder size on elongated grain growth in #beta#-Si_3N_4 ceramics[J].Journal of the European Ceramic Society,2000(14/15):2667-2671.
[8] S.-B. Li;H.-X. Zhai;G. P. Bei .Formation of Ti_3AlC_2 by mechanically induced self-propagating reaction in Ti-Al-C system at room temperature[J].Materials Science and Technology: MST: A publication of the Institute of Metals,2006(6):667-672.
[9] Z. J. Lin;M. J. Zhuo;Y. C. Zhuo .Microstructural characterization of layered ternary Ti_2AlC[J].Acta materialia,2006(4):1009-1015.
[10] J. W. Byeon;J. Liu;M. Hopkins .Microstructure and Residual Stress of Alumina Scale Formed on Ti_2AlC at High Temperature in Air[J].Oxidation of Metals,2007(1/2):97-111.
[11] P. Finkel;M. W. Barsoum;T. El-Raghy .Low temperature dependencies of the elastic properties of Ti_(4)AlN_(3), Ti_(3)Al_(1.1)C_(1.8), and Ti_(3)SiC_(2)[J].Journal of Applied Physics,2000(4):1701-1703.
[12] M. Radovic;M.W. Barsoum;A. Ganguly .On the elastic properties and mechanical damping of Ti_3SiC_2, Ti_3GeC_2, Ti_3Si_(0.5)Al_(0.5)C_2 and Ti_2AlC in the 300-1573 K temperature range[J].Acta materialia,2006(10):2757-2767.
[13] D.T. Wan;F.L. Meng;Y.C. Zhou .Effect of grain size, notch width, and testing temperature on the fracture toughness of Ti_3Si(Al)C_2 and Ti_3AlC_2 using the chevron-notched beam (CNB) method[J].Journal of the European Ceramic Society,2008(3):663-669.
[14] Y.C.Zhou;X.H.Wang .Deformation of polycrystalline Ti_2AlC under compression[J].Materials research innovations,2001(2):87-93.
[15] Y.W. Bao;W. Wang;Y.C. Zhou .Investigation of the relationship between elastic modulus and hardness based on depth-sensing indentation measurements[J].Acta materialia,2004(18):5397-5404.
[16] Z. Toth;A. Nagy;G. Steinbach .Investigation of indentation-caused cracking in surface-modified silica glasses[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2004(0):542-545.
[17] Y.W. Bao;X.H. Wang;H.B. Zhang .Thermal shock behavior of Ti_3AlC_2 from between 200 deg C and 1300 deg C[J].Journal of the European Ceramic Society,2005(14):3367-3374.
[18] H.B. Zhang;Y.C. Zhou;Y.W. Bao .Abnormal thermal shock behavior of Ti_3SiC_2 and Ti_3AlC_2[J].Journal of Materials Research,2006(9):2401-2407.
[19] D.B. Lee;S.W. Park .High-temperature oxidation of Ti_3AlC_2 between 1173 and 1473 K in air[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2006(1/2):147-154.
[20] Z.J. Lin;M.J. Zhuo;Y.C. Zhou .Interfacial microstructure of Ti_3AlC_2 and Al_2O_3 oxide scale[J].Scripta materialia,2006(10):1815-1820.
[21] H.J. Grabke .Oxidation of NiAl and FeAl[J].Intermetallics,1999(10):1153-1158.
[22] Z.SUN;Y.ZHOU;M.LI .HIGH TEMPERATURE OXIDATION BEHAVIOR OF Ti_3SiC_2-BASED MATERIAL IN AIR[J].Acta materialia,2001(20):4347-4353.
[23] M.P. BRADY;P.F. TORTORELLI .Alloy design of intermetallics for protective scale formation and for use as precursors for complex ceramic phase surfaces[J].Intermetallics,2004(7/9):779-789.
[24] M. P. Brady;P. F. Tortorelli;K. L. More;E. A. Payzant;B. L. Armstrong;H.-T. Lin;M. J. Lance;F. Huang;M. L. Weaver .Coating and near-surface modification design strategies for protective and functional surfaces[J].Materials and Corrosion,2005(11):748-755.
[25] X.H.Wang;Y.C.Zhou .Oxidation behavior of Ti_3AlC_2 powders in flowing air[J].Journal of Materials Chemistry: An Interdisciplinary Journal dealing with Synthesis, Structures, Properties and Applications of Materials, Particulary Those Associated with Advanced Technology,2002(9):2781-2785.
[26] F. L. MENG;Y. C. ZHOU;J. Y. WANG .Strengthening of Ti_2AlC by Substituting Ti with V[J].Scripta materialia,2005(12):1369-1372.
[27] J. X. Chen;Y. C. Zhou .Strengthening of Ti_3AlC_2 by incorporation of Al_2O_3[J].Scripta materialia,2004(6):897-901.
[28] J. Zhang;J.Y. Wang;Y.C. Zhou .Structure stability of Ti_3AlC_2 in Cu and microstructure evolution of Cu-Ti_3AlC_2 composites[J].Acta materialia,2007(13):4381-4390.
[29] M. Sundberg;G. Malmqvist;A. Magnusson .Alumina forming high temperature silicides and carbides[J].Ceramics International,2004(7):1899-1904.