利用锥形量热-傅里叶变换红外光谱联用仪对阻燃硬质聚氨酯泡沫材料(FRPU)在不同辐照强度下的火灾危险性进行了系统研究.研究结果表明,阻燃剂的加入能明显降低FRPU的热释放速率和总热释放量,但大大增大了FRPU的生烟速率、总生烟量和燃烧烟气中CO、HCN和HCl等有毒气体的生成量;随着辐照强度的增大,FRPU的热释放速率峰值、总热释放量、总生烟量和燃烧烟气中的CO、HCN和HCl浓度的最大值分别由131 kW/m2、8.0 MJ/m2、3.8 m2/m2、192.7 μL/L、42.7μL/L和77.4 μL/L增大到260 kW/m2、39.7 MJ/m2、13.8 m2/m2、734.5 μL/L、157.7 μL/L和210.5μL/L.
参考文献
[1] | S V levchik;E D Weil .Thermal decomposition,combustion and fire-retardancy of polyurethanes-a review of the recent literature[J].Polymer international,2004(11):1585-1610. |
[2] | D.K. Chattopadhyay;Dean C. Webster .Thermal stability and flame retardancy of polyurethanes[J].Progress in Polymer Science,2009(10):1068-1133. |
[3] | M. Checchin;C. Cecchini;B. Cellarosi .Use of cone calorimeter for evaluating fire performances of polyurethane foams[J].Polymer Degradation and Stability,1999(3):573-576. |
[4] | Anna A. Stec;T. Richard Hull .Assessment of the fire toxicity of building insulation materials[J].Energy and buildings,2011(2/3):498-506. |