对TA15钛合金电子束焊接试样进行充氢,研究了充氢对显微组织形态的影响,并对微量氢对TA15疲劳寿命影响进行考察.显微组织研究表明:充氢量低于0.105%(质量分数)时,氢以固溶态存在于合金中,并未形成氢化物.疲劳试验结果表明:随充氢量的增加,疲劳寿命大幅下降;这是由于微量氢的存在降低了TA15合金的韧性,固溶氢增加了疲劳裂纹的扩展速率,且氢通过影响裂纹尖端的性能加速疲劳裂纹扩展.焊缝区马氏体束呈团状结晶,且以团为单位统一变形,导致断口上呈团簇形态;且氢对马氏体团疲劳扩展中的行为有一定影响.

参考文献

[1] Lee C S;Margolin H .[J].Metallurgical Transactions Physical Metallurgy and Materials Science,1986,17A(03):451.
[2] Kolachev B A et al.[J].Metal Science and Heat Treatment,2003,45(3-4):127.
[3] Mal'kov A V.[J].Problemy Prochnosti,1984(03):73.
[4] Datta P K;Strafford K N;Dowson A L.Light Metals:Science and Technology[A].Aedermannsdorf,Switz:Trans Tech Publ,1985:203.
[5] Evans W J;Bache M R.Proceedings of 2nd International Conference on Fundamental Physical Aspects of the Strength of Crystalline Materials[C].Sandai:Japan Inst Metals,1994:493.
[6] Pao P S et al.[J].Journal of Nuclear Materials,1981,104:931.
[7] Bavarian B.TMS Annual Meeting[C].Warrendale:The Minerals,Metal and Materials Society,1993:105.
[8] Sommer A W;Froes F H;Eylon D.Proceedings of the 1987 TMS-AIME Annual Symposium[C].Warrendale:Metallurgical Society Inc,1987:55.
[9] Christ H J et al.[J].Fatigue & Fracture of Engineering Materials & Structures,1996,19(12):1421.
[10] Shipilov S A.[J].Metallovedeniei Termicheskaya Obrabotka Metallovb Metalloved,2001(01):31.
[11] Sarrazin-Baudoux C;Lesterlin S;Petit J.Proceedings of the 27th National Symposium on Fatigue and Fracture Mechanics[C].West Conshohoken:American Society for Testing and Materials,1997:117.
[12] Kolman D G;Scully J R.Proceedings of the Symposium of Effects of the Environment on the Initiation of Crack Growth[C].Conshohocken:American Society for Testing and Materials,1997:61.
[13] Willams D P;NelsonE H G .[J].Metallurgical and Materials Transactions,1972,3(08):2107.
[14] Yeh MS.;Huang JH. .Hydrogen-induced subcritical crack growth in Ti-6Al-4V alloy[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,1998(1/2):96-107.
[15] Lang M .[J].Acta Materialia,1999,47(11):3247.
[16] Fishgoit A V et al.[J].SOVIET MATERIALS SCIENCE,1983,19(05):29.
[17] 郭隆,白秉哲,侯红亮.置氢Ti-6Al-4V钛合金超塑性研究[J].稀有金属,2009(04):467-471.
[18] Pao P S et al.[J].Scripta Materialia,1998,40(01):19.
[19] Yoder G R;Cooley L A;Crooker T W .[J].Engineering Fracture Mechanics,1979,11(04):805.
[20] 李行志,胡树兵,肖建中,王亚军,李清华,籍龙波.TA15钛合金电子束焊接接头不同区域的疲劳裂纹扩展行为研究[J].航空材料学报,2010(01):52-56.
[21] Baeslack Ⅲ W A et al.[J].Welding Journal,1981,60(07):121.
[22] Zuo JH;Wang ZG;Han EH .Effect of microstructure on ultra-high cycle fatigue behavior of Ti-6Al-4V[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2008(1/2):147-152.
[23] Harvey S E et al.[J].Acta Metallurgica Et Materialia,1994,42(10):3493.
[24] Kim Y H et al.[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1978,9A(11):1679.
[25] Hack J E et al.[J].Metallurgical and Materials Transactions A:Physical Metallurgy and Materials Science,1982,13A(10):1729.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%