采用溶胶-凝胶法在Ti6Al4V基体上制备了HAP/TiO2纳米复合涂层,并引入TiO2作为缓冲层.使用XRD、FT-IR和FE-SEM协同EDS研究了450、550和650℃温度下煅烧后涂层的组成和结构特征.实验结果表明,HAP/TiO2涂层均具有较好的结晶态,涂层厚度均匀、致密,与金属基体结合紧密.由亚微米级HAP晶体颗粒(100~200nm)镶嵌在分布均匀的纳米TiO2胶质之中,TiO2凝胶颗粒大小随煅烧温度的变化在10~30nm变动.力学测试结果表明这些复合涂层具有较高的结合强度,随着煅烧温度的升高,涂层的抗拉强度呈现上升的趋势.体外生物活性的测试证实了它们的生物活性.

参考文献

[1] 储成林;朱景川;尹钟大.[J].功能材料,1999(06):606-609.
[2] Breme J.;Groh L.;Zhou Y. .DEVELOPMENT OF A TITANIUM ALLOY SUITABLE FOR AN OPTIMIZED COATING WITH HYDROXYAPATITE[J].Biomaterials,1995(3):239-244.
[3] 赵冰;杜荣归;林昌健.[J].功能材料,2001:126-129.
[4] Li P;De Groot K.[J].Journal of Biomedical Materials Research:1495-1500.
[5] Uchida M;Kim H M;Kokubo T.[J].Journal of the American Ceramic Society(12):2969-2974.
[6] Manso M;Langlet M;Fenandez M.[J].Materials Science and Engineering:451-454.
[7] Kim HW;Koh YH;Li LH;Lee S;Kim HE .Hydroxyapatite coating on titanium substrate with titania buffer layer processed by sol-gel method.[J].Biomaterials,2004(13):2533-2538.
[8] 郑学斌,周霞明,张叶方,丁传贤.等离子喷涂 HA/TiO2复合涂层[J].无机材料学报,1999(06):956-962.
[9] Hwang K;Lim Y.[J].Surface and Coatings Technology:172-175.
[10] Tkalcec E;Sauer M;Nonninger R.[J].Journal of Marter Sci:5253-5263.
[11] Liu DM;Yang Q;Troczynski T .Sol-gel hydroxyapatite coatings on stainless steel substrates.[J].Biomaterials,2002(3):691-698.
[12] Ben Nissan B;Milev A;Vago R .Morphology of sol-gel derived nano-coated coralline hydroxyapatite.[J].Biomaterials,2004(20):4971-4975.
[13] Li P;De Groot K;Kokubo T.[J].Journal of Sol-Gel Science and Technology:27-34.
[14] Milella E;Cosentino F;Licciulli A;Massaro C .Preparation and characterisation of titania/hydroxyapatite composite coatings obtained by sol-gel process.[J].Biomaterials,2001(11):1425-1431.
[15] Piveteau LD;Gasser B;Schlapbach L .Evaluating mechanical adhesion of sol-gel titanium dioxide coatings containing calcium phosphate for metal implant application.[J].Biomaterials,2000(21):2193-2201.
[16] Lim Y M;Park Y J;Yun Y H.[J].Ceramics International:37-41.
[17] Weng J.;Wolke JGC.;Zhang XD.;Degroot K.;Liu Q. .FORMATION AND CHARACTERISTICS OF THE APATITE LAYER ON PLASMA-SPRAYED HYDROXYAPATITE COATINGS IN SIMULATED BODY FLUID[J].Biomaterials,1997(15):1027-1035.
[18] 郭连峰,张文光,王成焘.纳米羟基磷灰石的制备及结晶尺寸的控制[J].无机化学学报,2004(03):291-296.
[19] 陈琦丽,唐超群,肖循.TiO2纳米微粒的溶胶-凝胶法制备及XRD分析[J].材料科学与工程,2002(02):224-226.
[20] Kokubo T. .FORMATION OF BIOLOGICALLY ACTIVE BONE-LIKE APATITE ON METALS AND POLYMERS BY A BIOMIMETIC PROCESS[J].Thermochimica Acta: An International Journal Concerned with the Broader Aspects of Thermochemistry and Its Applications to Chemical Problems,1996(0):479-490.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%