The microstructures and mechanical properties of the as-rolled Mg-3Li and Mg-3Li-1Sc (wt%) alloys before and after annealing treatment have been investigated. Results show that the grains are refined evidently and the recrystallization temperature is improved for more than 100℃by adding 1 wt% Sc into the Mg-3Li alloy. After complete recrystallization, both the strength and ductility of the Mg-3Li alloy are improved evidently with the addition of minor Sc. The brittle fracture tendency of Mg-3Li-ISc alloy also reduces obviously.
参考文献
[1] | Z. Drozd;Z. Trojanova;S. Kudela .Deformation behaviour of Mg-Li-Al alloys[J].Journal of Alloys and Compounds: An Interdisciplinary Journal of Materials Science and Solid-state Chemistry and Physics,2004(1/2):192-195. |
[2] | Z. Trojanova;Z. Drozd;P. Lukac .Deformation behaviour of Mg-Li alloys at elevated temperatures[J].Materials Science & Engineering, A. Structural Materials: Properties, Misrostructure and Processing,2005(0):148-151. |
[3] | D.K. Xu;L. Liu;Y.B. Xu;E.H. Han .The strengthening effect of icosahedral phase on as-extruded Mg–Li alloys[J].Scripta materialia,2007(3):285-288. |
[4] | W.A. Counts;M. Friak D. Raabe;J. Neugebauer .Using ab initio calculations in designing bcc Mg-Li alloys for ultra-lightweight applications[J].Acta materialia,2009(1):69-76. |
[5] | T. Liu;Y.D. Wang;S.D. Wu .Textures and mechanical behavior of Mg-3.3 percent Li alloy after ECAP[J].Scripta materialia,2004(11):1057-1061. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%