Exchange coupling and magnetic properties of SmCo5 alloys containing different amounts of Sn were investigated in sintered magnets. X-ray diffraction analysis revealed the formation of Sm2Co17 and Sm2Co7 phases in SmCo5 matrix. Exchange coupling mechanism was evaluated by switching field distribution, dc-demagnetization and magnetization curves as function of reverse applied field. Energy product of 59.2 kJ/m3 (7.4 MGOe), remanent magnetization to maximum magnetization ratio of 0.97 and remanence coercivity to intrinsic coercivity ratio of 1.75 were achieved for 0.2 at.% Sn.

参考文献

[1]
[2]
[3]
[4] E.F. Kneller and R. Hawig: IEEE Trans. Magn., 1991, 27(4), 3588.

[2 ] M. Ghidini, G. Asti, R. Pellicelli, C. Pernechele and M. Solzi: J. Magn. Magn. Mater., 2007, 316, 159.

[3 ] R.D. Shull, J. Iron Steel Res. Int., 2007, 14(4), 69.

[4 ] R. Skomski and J.M.D. Coey: Permanent Magnetism, Institute of Physics Publishing, Bristol and Philadelphia, 1999, 298.

[5 ] R. Skomski: J. Phys.: Condens. Matter., 2003, 15, R841.

[6 ] J.T. Elizalde Galindo, H.A. Davies and J.A. MatutesAquino: Mater. Charact., 2007, 58, 805.

[7 ] Z. Chen, Y. Zhang, G.C. Hadjipanayis, Q. Chen and B.M. Ma: J. Alloy. Compd., 1999, 287, 227.

[8 ] J.P. Liu, Y. Liu and D.J. Sellmyer: J. Appl. Phys., 1998, 83(11), 6608.

[9 ] J.S. Jiang, J.E. Pearson, Z.Y. Liu, B. Kabius, S. Trasobares, D.J. Miller, S.D. Bader, D.R. Lee, D. Haskel, G. Srajer and J.P. Liu: Appl. Phys. Lett., 2004, 85(22), 5293.

[10] G.C. Hadjipanayis: J. Magn. Magn. Mater., 1999, 200, 373.

[11] A. Bollero, O. Gut°
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%