对氮化硅摩擦磨损性能相关影响因素及磨损机制进行了总结归纳,系统介绍了氮化硅摩擦磨损性能与材料性能、环境因素(介质、温度、载荷)、配对摩擦副材料因素的相关研究进展,提出了目前研究存在的问题,并展望了氮化硅摩擦磨损性能研究趋势.
参考文献
[1] | 薛群基;刘惠文 .陶瓷摩擦学1.陶瓷的摩擦与磨损[J].摩擦学学报,2004,15(04):376. |
[2] | 石维佳,赵文英,王金刚.热等静压氮化硅陶瓷、钴铬15及钼50钢摩擦学研究[J].机械设计与制造,2004(05):95-98. |
[3] | 谢志鹏.结构陶瓷[M].北京:清华大学出版社,2011:428. |
[4] | Lange F F .Relation between strength,fracture energy,and microstructure of hot-pressed Si3N4[J].Journal of the American Ceramic Society,2006,56(10):518. |
[5] | Marchia J et al.Influence of additive system (Al2 O3-RE2-O3,RE=Y,La,Nd,Dy,Yb) on microstructure and mechanical properties of silicon nitride-based ceramics[J].Mater Res,2009,12(02):145. |
[6] | Zhu Xinwen et al.Influence of additive composition on thermal and mechanical properties of Si3N4 ceramics[J].Journal of Materials Research,2004,19(10):3270. |
[7] | 邹强,徐廷献,郭文利,薛义丹.Si3N4陶瓷烧结中烧结助剂的研究进展[J].硅酸盐通报,2004(01):81-84. |
[8] | Carrasquero E;Bellosi A et al.Characterization and wear behavior of modified silicon nitride[J].Int J Refractory Metal Hard Mater,2005,23(4-6):391. |
[9] | Zutshi A;Haber R A et al.Processing,microstructure,and wear behavior of silicon nitride hot-pressed with alumina and yttria[J].Journal of the American Ceramic Society,1994,77:883. |
[10] | Jae-Hee Kim;B. Venkata Manoj Kumar;Seong-Hyeon Hong .Fabrication of Silicon Nitride Nanoceramics and their Tribological Properties[J].Journal of the American Ceramic Society,2010(5):1461-1466. |
[11] | Hiroyuki Miyazaki;Hideki Hyuga;Yu-ichi Yoshizawa .Correlation of wear behavior and indentation fracture resistance in silicon nitride ceramics hot-pressed with alumina and yttria[J].Journal of the European Ceramic Society,2009(8):1535-1542. |
[12] | Wayne S F;Bulian S T et al.Microstructure and wear resistance of silicon nitride composites[J].Friction Wear Ceram,1994,4:261. |
[13] | 孟凡英,郭绍义,刘曾岭,李兴俊,张术永.氮化硅基陶瓷的摩擦磨损特性研究[J].浙江理工大学学报,2008(01):79-82. |
[14] | Carrapichano, JM;Oliveira, FJ;Silva, RF;Gomes, JR .Functionality diagrams for hybrid mechanical seals with silicon nitride rings[J].Journal of the American Ceramic Society,2005(8):2177-2180. |
[15] | Hideki Hyugaa;Mark I J et al.Influence of carbon fibre content on the processing and tribological properties of silicon nitride/carbon fibre composites[J].Journal of the European Ceramic Society,2004,24:877. |
[16] | Hideki Hyuga;Mark I. Jones;Kiyoshi Hirao .Tribological Behavior of a Si_3N_4/Carbon Short Fiber Composite under Water Lubrication[J].Journal of the American Ceramic Society,2004(4):699-702. |
[17] | Hideki Hyuga;Yu-ichi Yoshizawa;Kiyoshi Hirao .Tribological Behavior of Si3N4 and Si3N4/Carbon Fiber Composites Against Stainless Steel Under Water Lubrication for a Thrust-Bearing Application[J].International Journal of Applied Ceramic Technology - Ceramic Product Development and Commercialization,2008(2):111-118. |
[18] | 氮化硅陶瓷的摩擦磨损特性[J].兰州大学学报,1995(01):38. |
[19] | Hideki Hyuga;Mark I. Jones;Kiyoshi Hirao .Influence of Rare-Earth Additives on Wear Properties of Hot-Pressed Silicon Nitride Ceramics under Dry Sliding Conditions[J].Journal of the American Ceramic Society,2004(9):1683-1686. |
[20] | Hidcki Hyuga;Mark I. Jones;Kiyoshi Hirao .The Relationship Between Multiple Scratch Tests and Wear Behavior of Hot-Pressed Silicon Nitride Ceramics with Various Rare-Earth Additive Systems[J].Journal of the American Ceramic Society,2008(1):192-197. |
[21] | Carrapichano J M;Gomes J R et al.Si3N4 and Si3N4/SiC composite rings for dynamic sealing of circulating fluids[J].WEAR,2003,255:695. |
[22] | Shiro Kanasaki et al.Sealing boric acid solutions with mechanical seals in nuclear service[J].LUBRICATION ENGINEERING,1975,33(08):425. |
[23] | Vila M;Carrapichano J M et al.Ultra-high performance of DLC-coated Si3N4 rings for mechanical seals[J].WEAR,2008,265:940. |
[24] | Tome M A;Fernandes A J S et al.High performance sealing with CVD diamond self-mated rings[J].Diamond and Related Materials,2005,14:617. |
[25] | Camargo Jr S S;Gomes J R et al.Silicon-incorporated diamond-like coatings for Si3N4 mechanical seals[J].THIN SOLID FILMS,2005,482:221. |
[26] | 魏建军;薛群基 .氮化硅在水和乙醇中的摩擦化学机理研究[J].硅酸盐学报,1993,11(02):149. |
[27] | Gates R S;Hsu S M .Silicon nitride boundary lubrication:Lubrication mechanism of alcohols[J].Tribology Transactions,1995,38(03):645. |
[28] | 宋宝玉 .不同湿度气氛中氮化硅陶瓷的摩擦学性能[J].固体润滑,1989,9(08):175. |
[29] | Roberto C. Dante;C. K. Kajdas.A review and a fundamental theory of silicon nitride tribochemistry[J].Wear: an International Journal on the Science and Technology of Friction, Lubrication and Wear,2012:27-38. |
[30] | Kalin M;Vizintin J et al.Wear mechanisms in oil-lubricate d and dry fretting of silicon nitride against bearing steel contacts[J].WEAR,1997,210:27. |
[31] | Childs T H C;Mimaroglu A .Sliding friction and wear up to 600 ℃ of high speed steels and silicon nitrides for gas turbine bearings[J].WEAR,1993,163:156. |
[32] | 汪复兴;程荫芊 等.氮化硅陶瓷-金属摩擦副摩擦学性能研究[J].清华大学学报,1992,32(05):35. |
[33] | Saito T;Imada Y;Honda F .An analytical observation of the tribochemical reaction of silicon nitride sliding with low friction in aqueous solutions[J].WEAR,1997,205:153. |
[34] | Loffelbein B et al.Sliding friction and wear of ceramic in netural,acid and basic aqueous solutions[J].WEAR,1993,162-164:220. |
[35] | Dong X;Jahanmir S .Wear transition diagram for silicon nitride[J].WEAR,1993,165:169. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%