采用熔炼铸造方法制备出Mg-5%Hg-1%Ga合金,在573~773 K时效不同时间,利用X射线物相检测、扫描电镜结合能谱分析第二相Mg<,3>Hg的形貌和分布,用交流阻抗法等电化学方法研究Mg<,3>Hg对Mg-5%Hg-1%Ga阳极在3.5%NaCl(质量分数)溶液中电化学性能的影响.结果表明:时效时间从15 min延长至200 h时,Mg-5%Hg-1%Ga合金中α-Mg和Mg<,3>Hg的共晶组织转变为α-Mg基体中弥散分布Mg<,3>Hg颗粒,这种转变降低了浓差极化和法拉第反应中电荷传递电阻,提高电化学活性.弥散分布的Mg<,3>Hg颗粒使Mg-5%Hg-1%Ga合金组织均匀,提高了耐腐蚀性能.

参考文献

[1] Aurbach, D;Suresh, GS;Levi, E;Mitelman, A;Mizrahi, O;Chusid, O;Brunelli, M .Progress in rechargeable magnesium battery technology[J].Advanced Materials,2007(23):4260-4267.
[2] Renuka R .[J].Materials Chemistry and Physics,1999,59(01):42.
[3] Jerome Giraudet;Daniel Claves;Katia Guerin;Marc Dubois;Axel Houdayer;Francis Masin;Andre Hamwi .Magnesium batteries: Towards a first use of graphite fluorides[J].Journal of Power Sources,2007(1):592-598.
[4] Renuka R .[J].Journal of Applied Electrochemistry,1997,27(12):1394.
[5] Zhao H;Bian P;Ju D .[J].Journal of Environmental Sciences,2009,21(z1):S88.
[6] Aung N N;Zhou W .[J].Corrosion Science,2010,52(02):589.
[7] Lei W;Bo P Z;Tadashi S .[J].Materials & Design,2010,31(02):857.
[8] He M F;Liu L;Wu Y T et al.[J].Corrosion Science,2008,50(12):3267.
[9] The influence of the microstructure on the atmospheric corrosion behaviour of magnesium alloys AZ91D and AM50[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2010(3):1077.
[10] Muniyandi N;Mathur P B .[J].Corrosion,1991,27(01):68.
[11] R. Udhayan;Devendra Prakash Bhatt .On the corrosion behaviour of magnesium and its alloys using electrochemical techniques[J].Journal of Power Sources,1996(1):103-107.
[12] Feng Y;Wang R C;Yu K et al.[J].Journal of Alloys and Compounds,2009,473(1-2):215.
[13] Bagshaw N E;Warrell S.Power Sources:Research and Development in Non-Mechanical Electrical Power Sources[M].London:E-Publishing Inc,1981:117.
[14] Sammoura F;Lee K B;Lin L W .[J].Sensors and Actuators B: Chemical,2004,A(111):79.
[15] Uhlenhaut D I;Furrer A;Uggowitzer P J et al.[J].Intermetallics,2009,17(10):811.
[16] D.O. Flamini;S.B. Saidman;J.B. Bessone .Aluminium activation produced by gallium[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2006(6):1413-1425.
[17] 邓姝皓,易丹青,赵丽红,周玲伶,王斌,冀成年,兰博.一种新型海水电池用镁负极材料的研究[J].电源技术,2007(05):402-405.
[18] Shayeb EI H A;Abd EI F M;Abedin S Z E .[J].Corrosion Science,2001,43(04):643.
[19] Maria Nestoridi;Derek Pletcher;Robert J.K. Wood;Shuncai Wang;Richard L. Jones;Keith R. Stokes;Ian Wilcock .The study of aluminium anodes for high power density Al/air batteries with brine electrolytes[J].Journal of Power Sources,2008(1):445-455.
[20] Feng Y;Wang R C;Yu K et al.[J].Materials Transactions-Japan Institute of Metals,2008,49(05):1077.
[21] J.B. Bessone .The activation of aluminium by mercury ions in non-aggressive media[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2006(12):4243-4256.
[22] Pinssco M R;Angelini E;Cordano E et al.[J].Journal of Alloys and Compounds,2001,317-318(12):411.
[23] Rao K V .[J].Defence Science Journal,2001,51(02):161.
[24] Song G L;Andrej A .[J].Advances in Engineering Materials,1999,1(01):11.
[25] FENG Yan,WANG Ri-chu,PENG Chao-qun,WANG Nai-guang.Influence of Mg21Ga5Hg3 compound on electrochemical properties of Mg-5%Hg-5%Ga alloy[J].中国有色金属学会会刊(英文版),2009(01):154-159.
[26] Carroll W M;Breslin C B .[J].Corrosion Science,1992,33(07):1161.
[27] Khedr M G A;Lashien A M S .[J].Corrosion Science,1992,33(01):137.
[28] Cabot P L;Garrido J A;Perez E et al.[J].Electrochimica Acta,1995,40(04):447.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%