对先驱体硅树脂高温(1200℃)转化陶瓷接头连接Cf/SiC复合材料进行了研究.探讨了添加活性填料(纳米级Si,Al粉)后先驱体裂解所发生的反应趋势及重复浸渍-裂解过程对连接强度的影响.结果表明,通过添加活性填料纳米级Si,Al粉可以改善连接效果,但性能难以达到应用目标.通过重复浸渍2 g/mLSR249/ethanol溶液-裂解可以提高连接剪切强度.经过8个浸渍-裂解周期后,得到连接剪切强度达到64.24 MPa.
参考文献
[1] | Gause L W;Alper J .Mechanics of Composites,Review[R].Chio:Air Force Materials Laboratory,1983. |
[2] | 任家烈;吴爱萍.先进材料的连接[M].北京:机械工业出版社,2000 |
[3] | Colombo P.;Donato A.;Scarinci G.;Riccardi B. .Joining of SiC/SiCf ceramic matrix composites for fusion reactor blanket applications[J].Journal of Nuclear Materials: Materials Aspects of Fission and Fusion,2000(2/3):127-135. |
[4] | Colombo P.;Pippel E.;Woltersdorf J.;Sglavo V. .Joining of reaction-bonded silicon carbide using a preceramic polymer[J].Journal of Materials Science,1998(9):2405-2412. |
[5] | Pippel E;Woltersdorf J;Colombo P.[J].Journal of the European Ceramic Society,1997(17):1259. |
[6] | Sherwood W J;Whitmarsh C K;Jacobs J M et al.[J].Ceramic Engineering and Science Proceedings,1997,18(3A):177. |
[7] | 所俊,陈朝辉,韩卫敏,郑文伟.硅树脂高温转化陶瓷结合层连接陶瓷材料[J].硅酸盐学报,2005(03):386-390. |
[8] | 所俊,陈朝辉,郑文伟,韩卫敏.先驱体浓度、工艺温度及惰性填料对先驱体高温连接陶瓷材料性能的影响[J].航空材料学报,2006(01):40-45. |
[9] | 所俊,陈朝辉,郑文伟,韩卫敏.先驱体硅树脂高温连接Cf/SiC复合材料--惰性及活性填料对连接性能的影响[J].复合材料学报,2005(04):35-39. |
[10] | 时均;汪家鼎;余国琮.化学工程手册[M].北京:化学工业出版社,2002:1. |
[11] | Dean J A.Lange's Handbook of Chemistry[M].北京:科学出版社,2002 |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%