利用激光拉曼方法直接测量SiC(f)/Ti-22Al-26Nb复合材料中SiC纤维表面C涂层的拉曼吸收光谱,由此计算出复合材料的残余应力,并对复合材料的残余应力进行有限元模拟计算分析.结果表明:复合材料界面反应层起到降低残余应力的作用,反应层越厚残余应力降低值越大,试验结果与模拟计算结果基本一致.
参考文献
[1] | Fang Q.;Hocking MG.;Zhang JY.;Sidky PS. .Cracking behaviour of carbon coating on SiC fibre and residual stresses in Ti/SiC MMCs[J].Surface & Coatings Technology,1998(1/3):264-270. |
[2] | 杨延清,朱艳,陈彦,张清贵,张建民.SiC纤维增强Ti基复合材料的制备及性能[J].稀有金属材料与工程,2002(03):201-204. |
[3] | Akser E O;Choy K L .[J].Composites Part A:Applied Science and Manufacturing,2001,32:243. |
[4] | Fang Q;Sidky P S;Hocking G M .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2000,288:293. |
[5] | Rangaswamy P;Bourke a M A M;Wright b P K .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,1997,224:200. |
[6] | Rangaswamy P;Revelos W C;Jayaraman N .[J].Journal of Compos TechnolRes,1994,16(01):47. |
[7] | Rangaswamy P;Jayaraman N .[J].Journal of Composites Technology and Research,1995,17(01):43. |
[8] | Rangaswamy P;Bourke M A M;Wright P K et al.[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,1997,224:200. |
[9] | Saigal A;Kupperman D S;Majumdar S .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,1992,150:59. |
[10] | Yanling Warda;Robert Young J .[J].Composites Part A:Applied Science and Manufacturing,2002,33:1409. |
[11] | Yang X;Young R J .[J].Br Ceram J,1994,93:1. |
[12] | Day R J;Piddock V;Taylor R et al.[J].Journal of Materials Science,1989,24:2898. |
[13] | Meinhard K;Bernhardr M;Georg G .[J].Journal of the American Ceramic Society,1993,76:2607. |
[14] | Huang Bin;Yang Yanqing .[J].Materials Science and Engineering A:Structural Materials Properties Microstructure and Processing,2008,489:178. |
[15] | Yanling Ward;Robert J .[J].Journal of Materials Science,2001,36:55. |
[16] | Zong G et al.[J].Mar Scri Metal,1993,29:88. |
[17] | Colomban P H;Gouadec G;Mathez J et al.[J].Composites Part A:Applied Science and Manufacturing,2006,37:646. |
[18] | Masse P;Cavrot J P;Depecker C et al.[J].Macromolecular Symposia,1995,94:249. |
[19] | Kawagoe M;Hashimoto S;Nomiya M et al.[J].Journal of Raman Spectroscopy,1999,30:913. |
[20] | Soon-Eng Ong;Sam Zhang;Hejun Du .Relationship between bonding structure and mechanical properties of amorphous carbon containing silicon[J].Diamond and Related Materials,2007(8):1628-1635. |
[21] | Gwéna(e)l Gouadec;Philippe Colomban Prog .[J].Cry Grow & Char Mat,2007,53:39. |
[22] | Gouadec G;Karlin S;Colomban P H .[J].Composites Part B:Engineering,1998,29B:251. |
[23] | Yang Y Q;Zhu Y .[J].Scripta Materialia,2004,51:385. |
上一张
下一张
上一张
下一张
计量
- 下载量()
- 访问量()
文章评分
- 您的评分:
-
10%
-
20%
-
30%
-
40%
-
50%