将柔性链聚乙烯醇(PVA)分别与刚性链天然高分子海藻酸钠(SA)和壳聚糖(CS)共混,以增强其柔韧性及双极膜界面层的相容性。然后分别以纳米无机半导体材料和戊二醛为交联剂,对PVA/SA和PVA/CS进行改性,制备了PVA-mSA/mCS双极膜。测定了双极膜的J-V曲线、膜阻抗、接触角和溶胀度。以扫描电镜对PVA-ZnO-SA/mCS膜成分与形貌作表征,膜厚约121μm,中间界面层厚约5μm。电子能谱图表明氧化锌均匀分布在阳膜层中。实验结果表明,采用纳米ZnO改性后双极膜的亲水性增强,具有更强的中间界面层水解离能力,较小的工作电压和较低的膜阻抗,可以广泛应用于绿色化学和环境治理。

Polyvinylchloride(PVC)-mSA/mCS bipolar membrane(BPM) was prepared by the paste method.PVA/sodium alginate(SA) and PVA /chitosan(CS) were cross-linked by inorganic nano-materials and glutaraldehyde(GA),respectively.SEM photographs show that PVA-ZnO-SA/mCS BPM is consists of anion layer and cation layer,the thickness of the BPM is 121 μm,the interface of BPM is 5 μm.Electronic spectrum(EDS) indicates that ZnO well-distributed in cation layer.J-V curve and AC impedances of BPMs were investigated.It can be seen that PVA-ZnO-SA/mCS BPM shows lower working voltage,smaller membrane impedance,and ideal nano-ZnO modification effect.In addition,the dopping nano-ZnO improves the hydrophilic property and mechanical properties of the BPM.Therefore,PVA-ZnO-SA/mCS is an excellent BPM and can be widely used in the green chemistry and environmental management.

参考文献

[1] 周红军,容敏智,章明秋,阮文红.纳米SiO2/聚丙烯复合材料的反应性增容[J].高分子学报,2007(02):158-164.
[2] 王平华,严满清.聚丙烯/PMMA/CaCO3纳米复合材料的制备、结构与力学性能[J].应用化学,2003(11):1066-1070.
[3] 黄怀国.ZnO/PANI复合膜的制备和光电化学研究[J].矿冶工程,2006(04):50-53,57.
[4] Hosono T.;Tanioka A. .Effect of polymer composition in intermediate layer on water splitting in bipolar membranes[J].Polymer: The International Journal for the Science and Technology of Polymers,1998(18):4199-4204.
[5] 熊明娜,周树学,陈辉,武利民.溶胶-凝胶法制备丙烯酸树脂/TiO2有机-无机杂化材料及其结构表征[J].高分子学报,2005(03):417-422.
[6] Xu CX;Chen RY;Zheng X;Chen X;Chen Z .Preparation of PVA-GA-CS/PVA-Fe-SA bipolar membrane and its application in electro-generation of 2,2-dimethyl-3-hydroxypropionic acid[J].Journal of Membrane Science,2008(2):218-224.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%