高级检索

研究了沸水封闭、醋酸镍封闭和电压加载下己二酸铵封闭对LY12铝合金阳极氧化膜耐蚀性的影响。通过场发射扫描电镜(FE-SEM)和电化学阻抗谱(EIS)对三种无铬封闭方法处理后铝合金阳极氧化膜的表面微观形貌和耐蚀性进行了研究。结果表明:封闭处理可以有效地闭合阳极氧化膜的微孔,提高氧化膜耐腐蚀性能。电压加载下己二酸铵封闭可以有效缓解氧化膜的腐蚀。三种无铬封闭方法处理后的氧化膜耐腐蚀性能从小到大依次为:沸水封闭,醋酸镍封闭,电压加载下己二酸铵封闭。

Effects of boiling water sealing,nickel acetate sealing and ammonium adipate sealing under voltage loading on corrosion resistance of anodic oxide films on LY12 aluminum alloy were studied.Surface morphology and corrosion resistance of the anodic oxide films on aluminum alloy sealed by the three chromium-free methods were studied by means of field emission scanning electron microscopy(FE-SEM) and electrochemical impedance spectroscopy(EIS).The results show that pores of the anodic oxide films are closed after sealing.Ammonium adipate sealing under voltage loading can improve significantly corrosion resistance of the anodic oxide films.Corrosion resistance of the anodic oxide films sealed by three chromium-free methods increases in the following order:boiling water sealing,nickel acetate,ammonium adipate sealing under voltage loading.

参考文献

[1] Hao L;Cheng B R .Sealing processes of anodic coatlngs-past,present,and future[J].Aluminum Finishlng,2000,12(08):8-18.
[2] 田连朋,左禹,赵景茂,熊金平,赵旭辉.铝合金阳极氧化膜醋酸镍封闭方法耐蚀性研究[J].腐蚀与防护,2006(02):58-62.
[3] 李凌杰,雷惊雷,李荻,蔡生民,朱国伟,雷向利.铈、锂盐对铝阳极氧化膜的协同封闭作用[J].物理化学学报,2003(10):922-926.
[4] Bautista A.;Gonzalez JA.;Lopez V. .Influence of triethanolamine additions on the sealing mechanism of anodised aluminium[J].Surface & Coatings Technology,2002(1):49-54.
[5] 赵景茂,王珊珊,郭超,赵旭辉,左禹.铝合金阳极氧化膜双向脉冲封闭工艺[J].北京化工大学学报(自然科学版),2008(01):54-57.
[6] Gregory B;Nadine P;Catherine D et al.FESEM and EIS study of sealed AA2024 T3 anodized in suffuric acid electrolytes:Influence of tartaric acid[J].Journal of the Electrochemical Society,2008,155(11):C521-C529.
[7] V. Lopez;M. J. Bartolome;E. Escudero .Comparison by SEM, TEM, and EIS of Hydrothermally Sealed and Cold Sealed Aluminum Anodic Oxides[J].Journal of the Electrochemical Society,2006(3):B75-B82.
[8] Degradation of the corrosion resistance of anodic oxide films through immersion in the anodising electrolyte[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2010(7):2219.
[9] Boisier, G;Lamure, A;Pebere, N;Portail, N;Villatte, M .Corrosion protection of AA2024 sealed anodic layers using the hydrophobic properties of carboxylic acids[J].Surface & Coatings Technology,2009(22):3420-3426.
[10] S. Feliu;J. A. Gonzalez;V. Lopez .Characterisation of porous and barrier layers of anodic oxides on different aluminium alloys[J].Journal of Applied Electrochemistry,2007(9):1027-1037.
[11] Landry C C;Papp6 N;Mason M R et al.From minerals to materials:synthesis of alumoxanes from the reaction of boehmite with carboxylic acids[J].Journal of Materials Chemistry,1995,5(02):331-338.
[12] Kevin D D;A James M .In situ infrared spectroscopic analysis of the adsorption of aliphatic carboxylic acids to TiO2,ZrO2,Al2O3,and Ta2O3 from aqueous solutions[J].Spectrochimica Acta, Part A: Molecular and Biomolecular Spectroscopy,1999,55(7-8):1395-1405.
[13] Thompson GE. .POROUS ANODIC ALUMINA - FABRICATION, CHARACTERIZATION AND APPLICATIONS[J].Thin Solid Films: An International Journal on the Science and Technology of Thin and Thick Films,1997(1/2):192-201.
[14] Hitzig J;Junttner K;Lorentz W J .AC-impedance measurements on corroded porous aluminum oxide films[J].Journal of the Electrochemical Society,1986,133(05):887-892.
[15] Yuelong Huang;Hong Shih;Huochuan Huang;John Daugherty;Shun Wu;Sivakami Ramanathan;Chris Chang;Florian Mansfeld .Evaluation Of The Corrosion Resistance Of Anodized Aluminum 6061 Using Electrochemical Impedance Spectroscopy (eis)[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2008(12):3569-3575.
[16] Corrosion evaluation of microarc oxidation coatings formed on 2024 aluminium alloy[J].Corrosion Science: The Journal on Environmental Degradation of Materials and its Control,2010(8):P.2687.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%