采用硝酸铋[Bi(NO3)3·5H2O]、硝酸锶[Sr(NO3)2]、硝酸铁[Fe(NO3)3·9H2O]和乙醇铌[Nb(OC2H5)5]作为起始原料,乙二醇甲醚[C3H8O2]作为溶剂配制掺Fe的SrBi2Nb2O9前驱体溶液,利用溶胶-凝胶法在石英衬底上制备出0.1BiFeO3-0.9SrBi2Nb2O9铁电薄膜.研究了该薄膜的表面形貌、组分、晶体结构和光学性质.结果表明,经400℃退火后薄膜为非晶结构,而在空气中经600℃退火1h后,沉积的薄膜晶化成钙钛矿结构.制备的薄膜表面平整,颗粒分布均匀,表现出良好的光透过性,该薄膜的光学能隙大约为2.5eV.

参考文献

[1] Gu H S;Kuang A X;Wang S M et al.[J].Applied Physics Letters,1996,68(09):1209-1211.
[2] Scott J F;Ramesh R.Thin Film Ferroelectric Materials and Devices[M].MA:Kluwer Norwell,1997:115.
[3] Wu Y;Cao G Z .[J].Applied Physics Letters,1999,75:2650-2654.
[4] Haoshuang Gu;Junmin Xue;John Wang .Significant dielectric enhancement in 0.3BiFeO_(3)-0.7SrBi_(2)Nb_(2)O_(9)[J].Applied physics letters,2001(13):2061-2063.
[5] Gu H S;Zhang T J;Xue J M et al.[J].Materials Science and Engineering B,2003,99:116-120.
[6] Zhang ZG.;Wang YN.;Zhu JS.;Yan F.;Chen XB.;Shen HM.;Liu JS. .Fatigue characteristics of SrBi2Ta2O9 thin films prepared by metalorganic decomposition[J].Applied physics letters,1998(6):788-790.
[7] Lettieri J;Zurbuchen M A;Jia Y et al.[J].Applied Physics Letters,2000,76:2937-2939.
[8] S. Bhattacharyya;S. S. N. Bharadwaja;S. B. Krupanidhi .Alternating current conduction behavior of excimer laser ablated SrBi_(2)Nb_(2)O_(9) thin films[J].Journal of Applied Physics,2000(7):4294-4302.
[9] Zanetti S M;Leite E R;Longo E .[J].Journal of the European Ceramic Society,1999,19:1409-1412.
[10] Aizawa K;Tokumitsu E;Okamoto K .[J].Applied Physics Letters,2000,76:2609-2611.
[11] Gu HS.;Xue JM.;Gao XS.;Wang J. .Doping effects of BiFeO3 in layered perovskite SrBi2Nb2O9[J].Materials Chemistry and Physics,2002(1/3):105-109.
[12] Hodes G;Yaron A A;Decker F et al.[J].Physical Review B,1987,36:4215-4221.
上一张 下一张
上一张 下一张
计量
  • 下载量()
  • 访问量()
文章评分
  • 您的评分:
  • 1
    0%
  • 2
    0%
  • 3
    0%
  • 4
    0%
  • 5
    0%