ACTIVATION OF TiFe-LaNi_5 COMPOUND PARTICLES

(State Key Laboratory of RSA , Institute of Metal Research , Chinese Academy of Sciences , Shenyang 110015 , China)(Shenyang Institute of Technology , Shenyang 110015 , China)

金属学报(英文版)

Through controlled mechanical alloying treatment, TiFe and LaNi5 particles combined together on the surface of TiFe. This kind of compound particles can be easily activated at room temperature and an H2-pressure of 4.0 MPa. LaNi5 particles provided "window" and "path" for entrance of hydrogen from the surface to the interior of TiFe alloy.

关键词: TiFe-LaNi_5 compound particle , null , null

Guangzhou Institute of Energy Conversion,The Chinese Academy of Sciences,Guangzhou 510070,China

B.W. Wang , H. Shen

金属学报(英文版)

Ni-Cr System solar selective thin solid films were prepared by d.c. magnetron reactivesputtering under the atmosphere of O2 and N2. Ni-Cr alloy was chosen as targetmaterial and copper sheets as substrate. Using SEM, Spectrophotometer and Talystepto analyze the relations between the selective characteristic and the structure, theformation and the thickness of the thin films. The aim is to obtain good solar selectivethin films with high absorptance and low emittance, which is applied to flat plate solarheat collectors.

关键词: solar selective thin film , null , null , null

The effect of environmental variables on atmospheric corrosion of carbon steel in Shenyang

Chinese Science Bulletin

A study was carried out in order to investigate the effect of contaminants and meteorological variables on the rust layer of carbon steel exposed in Shenyang urban atmosphere. Seven kinds of contaminants and twelve kinds of meteorological parameters were also registered in order to correlate the data with respect to corrosion rate and the stepwise multiple regression analysis was carried out in order to obtain the best regression model. The sum of rainfall time as well as sunshine time and the concentration of H(2)S could stimulate initial atmospheric corrosion of carbon steel. The initial atmospheric corrosion kinetics of carbon steel was observed to follow the cubic equation. The corrosion products were analyzed by XRD and the transformation of phases in different periods was discussed.

关键词: contaminants;meteorological parameters;carbon steel;urban atmospheric;corrosion;stepwise multiple regression;corrosion products;rust;pollution