X. G. Bao
,
D. N. He
,
D. Lu
,
C. X. Li
,
J. L. Cheng and J. Y. Jiang( 1) National Mold and Dies CAD Engineering Research Center
,
Shanghai 200030
,
China 2) Shanghai Volkswagen Automotive Company Ltd.(SVW)
,
Shanghai 201805
,
China)
金属学报(英文版)
Taking CPU time cost and analysis accuracy into account, dynamic explicit finite ele- ment method is adopted to optimize the forming process of autobody panels that often have large sizes and complex geometry. In this paper, for the sake of illustrating in detail how dynamic explicit finite element method is applied to the numerical simulation of the autobody panel forming process,an example of optimization of stamping process pain meters of an inner door panel is presented. Using dynamic explicit finite element code Ls-DYNA3D, the inner door panel has been optimized by adapting pa- rameters such as the initial blank geometry and position, blank-holder forces and the location of drawbeads, and satisfied results are obtained.
关键词:
dynamic explicit finite element method
,
null
,
null
,
null
孙智
,
谢建军
,
王宇
,
施鹰
,
雷芳
人工晶体学报
采用溶胶-凝胶法结合旋涂工艺在单晶硅(111)上制备了Tb3+离子不同掺杂浓度的硅酸镥光学薄膜(Tb∶Lu2SiO5),利用热重差热分析(TG-DSC)、X射线衍射(XRD)、傅里叶红外光谱仪(FTIR)、原子力显微镜(AFM)和紫外可见荧光光谱(PL)对Tb∶Lu2SiO5薄膜的不同温度热处理的结构演变和发光性能进行了表征.研究结果表明Tb∶Lu2SiO5光学薄膜表面均匀、平整、无裂纹,薄膜样品从800℃开始晶华,1100 ℃时晶化完全.Tb∶Lu2SiO5的发光性能表现为Tb3+离子的4f→5d和5D4(5D3)→7FJ(J =6,5,4,3)跃迁结果(监测波长分别为480~650 nm和350~470 nm),激发主峰位于~240 nm,发射光谱主峰为542 nm的绿光发射.研究表明Tb3掺杂浓度对Tb∶Lu2SiO5光学薄膜的发光强度会产生明显影响,掺杂15mol%的Tb3+时,Tb∶Lu2SiO5薄膜的发光强度最强.
关键词:
Sol-gel法
,
Tb∶Lu2SiO5光学薄膜
,
结构演变
,
发光性能
孙丹丹
,
潘尚可
,
任国浩
,
吴云涛
,
商珊珊
,
张国庆
无机材料学报
doi:10.3724/SP.J.1077.2013.12735
针对Ce:Li6Lu(BO3)3晶体有效原子序数(zeff)高的问题,采用低原子序数的Y3+离子部分置换晶体中的Lu3+离子.通过固相合成法制备了Ce:Li6Lu1-xYx(BO3)3(0≤x≤1)固溶体.X射线粉末衍射(XRD)分析表明,该系列固溶体结构与Li6Gd(BO3)3晶体相同,空间群为P21/c.其X射线激发发射(XSL)的发光强度随着Y3+的含量增加而降低,当x=0.5时,固溶体的有效原子序数与Li6Gd(BO3)3闪烁体相当,但XSL发光强度是其1.4倍.Ce:Li6Lu0.5Y0.5(BO3)3的XSL光谱和PL光谱都在400 nm附近出现Ce3+离子的特征峰,可拟合出361和419 nm两个发光分量,分别对应于Ce3+离子的激发态电子的5d1→2F5/2和5d1→2F7/2能级跃迁.Ce:Li6Lu0.5Y0.5(BO3)3固溶体的衰减时间比Ce:Li6Lu(BO3)3略长,为19.6 ns.当x=0.50~0.70时,Ce:Li6Lu1-xYx(BO3)3(0≤x≤1)闪烁体比较适合作为中子探测材料.
关键词:
固相合成
,
Ce∶Li6LU1-xYx(BO3)3
,
X射线激发发射谱
,
PL光谱
,
衰减时间
李金凯
,
滕鑫
,
曹丙强
,
刘宗明
无机材料学报
doi:10.15541/jim20150479
以尿素为沉淀剂,通过均匀沉淀技术制备前驱体颗粒,经后续煅烧获得分散性能良好的球形(Lu0.95Eu0.05)3Al5O12((Lu0.95Eu0.05)AG)荧光颗粒.通过调整尿素浓度实现了球形荧光颗粒尺寸的可控合成.在此基础上,采用FT-IR、TG/DTA、XRD、FE-SEM、TEM和PLE/PL对材料的合成、物相形成及荧光性能等进行一系列表征.分析结果表明:前驱体经较低的温度1100℃煅烧即可获得(Lu0.95Eu0.05)AG球形荧光颗粒,且该荧光颗粒具有高的理论密度,适于闪烁体材料的应用.在235 nm电荷迁移带(CTB)的激发下,(Lu0.95Eu0.05)AG石榴石于592 nm(Eu3+的5D0→7F1磁偶极子跃迁)处呈现优异的橙红光发射,其色坐标为(0.63,0.37).该荧光颗粒的发光强度随颗粒尺寸的增大而增强,荧光寿命随颗粒尺寸的增大而缩短.球形(Lu0.95Eu0.05)AG石榴石颗粒有望成为一类新型荧光材料,广泛应用于照明及显示领域.
关键词:
Lu3Al5O12石榴石
,
Eu3+掺杂
,
球形颗粒
,
荧光性能
洪智亮
,
成来飞
,
鲁琳静
,
张立同
,
王一光
无机材料学报
doi:10.3724/SP.J.1077.2010.00186
采用溶胶-凝胶法制得三种镥硅酸盐体系粉体材料. 以氧化物的摩尔比来表示此三种粉体, 分别为:Lu2O3·SiO2、Lu2O3·2SiO2和Lu2O3·2.26SiO2. 在1400℃、50%H2O-50%O2静态常压气氛下, 研究了它们的耐水蒸气腐蚀性能.以单位面积重量变化率表征材料的耐水蒸气腐蚀性能, 结合X射线衍射(XRD)、傅里叶红外光谱(FTIR)和扫描电镜能谱分析(SEMEDS)等分析手段, 揭示了镥硅酸盐体系在高温水蒸气环境中的腐蚀机制和反应机理. 结果表明:三种原始粉体主要物相依次为:Lu2SiO5+Lu2Si2O7、 Lu2Si2O7+SiO2和Lu2Si2O7+SiO2. 在水蒸气作用下, Lu2SiO5相与Al2O3反应生成新相Lu3Al5O12, 而Lu2Si2O7相并未受到水蒸气的作用而发生任何反应, 表现出优异的化学稳定性.
关键词:
Lu2SiO5
,
Lu2Si2O7
,
environmental barrier coating (EBC)
,
water vapor corrosion
洪智亮
,
成来飞
,
鲁琳静
,
张立同
,
王一光
无机材料学报
doi:10.3724/SP.J.1077.2010.00186
采用溶胶-凝胶法制得三种镥硅酸盐体系粉体材料.以氧化物的摩尔比来表示此三种粉体,分别为:Lu_2O_3·SiO_2、Lu_2O_3·2SiO_2和Lu_2O_3·2.26SiO_2.在1400℃、50%H_2O-50%O_2静态常压气氛下,研究了它们的耐水蒸气腐蚀性能.以单位面积重量变化率表征材料的耐水蒸气腐蚀性能,结合X射线衍射(XRD)、傅里叶红外光谱(FTIR)和扫描电镜能谱分析(SEM-EDS)等分析手段,揭示了镥硅酸盐体系在高温水蒸气环境中的腐蚀机制和反应机理.结果表明:三种原始粉体主要物相依次为:Lu_2SiO_5+Lu_2Si_2O_7、Lu_2Si_2O_7+SiO_2和Lu_2Si_2o_7+SiO_2.在水蒸气作用下,Lu_2SiO_5相与Al_2O_3反应生成新相Lu_3Al_5O_(12)而Lu_2Si_2O_7相并未受到水蒸气的作用而发生任何反应,表现出优异的化学稳定性.
关键词:
Lu_2SiO_5
,
Lu_2Si_2O_7
,
环境障碍涂层
,
水蒸气腐蚀
马畅
,
李晓东
,
董宇
,
刘绍宏
,
朱琦
,
李继光
,
霍地
,
孙旭东
中国稀土学报
doi:10.11785/S1000-4343.20130411
以Lu(NO3)3和尿素为原料,采用均相沉淀法合成镥盐前驱体,研究Lu3+浓度、尿素/Lu3+摩尔比R对前驱体形貌的影响.结果表明,在反应温度为95℃时,低Lu3+浓度有利于单分散球形粉体的合成,并且适当的调整R值可将单分散球形颗粒尺寸控制在180 ~ 270 nm之间.在此基础之上,研究Eu3+掺杂Lu2O3单分散球形荧光粉体的合成,探讨了Eu3+的掺杂量(1%,3%,5%,7%,9%(原子分数))及煅烧温度(600~ 1200℃)对颗粒形貌及其荧光性能的影响.结果表明,Eu3+的掺杂使所得(Lu,Eu)盐前驱体颗粒尺寸远小于单纯的Lu盐前驱体,且Eu含量对荧光粉的荧光强度有着显著的影响,荧光淬灭浓度为5%.在考察的煅烧温度范围内,荧光粉的荧光强度随煅烧温度的提升而增强.
关键词:
Lu2O3
,
Eu3+
,
均相沉淀
,
单分散球形
,
前驱体
,
荧光性能
,
稀土
Journal of Magnetism and Magnetic Materials
Magnetization curves of the ternary tetragonal compound Lu2Fe14C were measured in an extracting-sample magnetometer in the temperature range from 1.5 to 300 K. The temperature dependence of the magnetic properties of Lu2Fe14C is discussed.
关键词:
anisotropy