Fluorescent Labeling of Nanometer Hydroxyapatite

Yuan ZHANG , Yuan YUAN , Changsheng LIU

材料科学技术(英文)

A novel surface treatment method using 3-aminopropyltriethoxysilane (AMPTES), was developed to immobilize the fluorescein molecule on nano-HAP (nanometer hydroxyapatite) powders. By pretreating the nano-HAP powders surface with AMPTES, fluorescein, chosen on the basis of the chemical structure of the nano- HAP powders, could be bound to the nano-HAP powders surface. The chemical compositions of nano-HAP before and after being labeled were characterized by Fourier transform infrared spectroscopy (FTIR) and X-ray photoelectron spectroscopy (XPS). The morphology, phase composition, and the fluorescence characteristics of the nano-HAP powders with and without staining were also investigated. The FTIR and XPS results revealed that fluorescein had been successfully immobilized on the surface of AMPTES-bound nano-HAP powders via the acylamide bond formation between the -COOH of fluorescein and the -NH2 of AMPTES. The labeled nano-HAP powders possessed strong fluorescent intensity with a little deviation from the maximum emission wavelength of fluorescein. But the morphology and phase composition had no obvious alteration. Under fluorescence microscopy, the labeled nano-HAP powders, even after 24 h cell incubation, exhibited strong fluorescence.

关键词: Nano-HAP , null , null , null

Intensified alkaline leaching pretreatment of refractory gold concentrates at common temperature and pressure

Transactions of Nonferrous Metals Society of China

A new process for the hydrometallurgy of refractory gold concentrates was presented. The process comprises grinding-leaching, intensified alkaline leaching (IAL), cyanidation and adsorption. In a stirring-type pulverizing-leaching tower mill, the concentrate is ground to <35. 6 μm of 95. 5 % while simultaneously leached by NaOH of 12 kg/t, then carried out intensified alkaline leaching for 48 h by NaOH of 108 kg/t in enhanced agitation tanks with the pulp concentration of 40% solids at the environmental temperature of 9. 5 &SIM; 13. 5 &DEG;C and the environmental pressure of 10(5) Pa. The oxidation rate of As is 94. 9%, and 47. 6% for S. The total consumption of NaOH is only 20% of that theoretically calculated under the conditions of full oxidation at the same oxidation rates of arsenic to arsenate and sulfur to sulfate. The gold leaching rate by NaCN in 24 h is increased from 9. 2% before pretreatment to 94. 2%. The consumption of NaCN is 7. 5 kg/t, which is one times less than that before pretreatment. The extraction cost of gold is about 422 Yuan/t.

关键词: refractory gold concentrates;grinding-leaching;intensified alkaline;leaching (IAL);pretreatment;common temperature and pressure