MICROSTRUCTURAL MODEL OF GATORIZED WASPALOY IN THE ISOTHERMAL FORGING PROCESS

J.P. Hu

金属学报(英文版)

A microstructural model, which was used to predict the evolution of microstrncturi of Gatorized Waspaloy in the isotherrnal forging process, was developed in terms of dynamic recrystallization and grain growth. Three steps of experiment were conducted during developing the model: (1) Specimens were compressed in MTS testiny machinci (2) Dynamic recrystallization and grain growth were discussed; (3) Dynamic reerys tallization model and grain growth model were set up. The agreement of simulated results and experimental data is fine.

关键词: Gatorized Waspaloy , null , null , null

pp和p碰撞中J/ψ的光生过程(英文)

朱佳庆 , 何俊伟 , 李云德

原子核物理评论

计算了pp和p碰撞中J/ψ的领头阶光生过程的产额。运用非相对论量子色动力学回顾了重夸克偶素产生的色单态机制与色八重态机制,并将它们分别用于处理直接光子过程和分解光子过程。通过与J/ψ产生的领头阶结果的对比可以看出,光生过程对J/ψ产额的修正在大横动量区域变得明显。

关键词: 光生过程 , 大横动量区域 , 重夸克偶素

J4不锈钢及化学镀Ni-P和Ni-Cu-P镀层在液-固两相流中的冲刷腐蚀行为

方信贤白允强王章忠

金属学报 doi:10.3724/SP.J.1037.2009.00499

用质量损失法系统研究了不同温度(25和50℃)和不同冲刷速率(0.63-1.88 m/s)下,J4不锈钢、Ni-P和Ni-Cu-P合金镀层, 及对比材料316L不锈钢在液-固两相流(20% H2SO4+20 g/L Al2O3)中的冲刷腐蚀行为. 结果表明:不锈钢和镀层的抗冲刷腐蚀性能由高到低依次为镀态Ni-Cu-P, 镀态Ni-P,热处理态Ni-Cu-P, 316L, J4. 提高两相流介质温度均使它们的冲刷腐蚀速率增大. 316L不锈钢在25℃液-固两相流介质中的冲刷腐蚀速率分别为镀态Ni-Cu-P, 镀态Ni-P和热处理态Ni-Cu-P镀层的8.5倍, 8倍和2.6倍以上, 而在50℃下分别为392倍, 80倍和14.8倍以上; J4不锈钢在25和50℃液-固两相流介质中的冲刷腐蚀速率分别为316L不锈钢的28倍和13倍以上. 在25和50℃, J4不锈钢分别为选择性腐蚀和均匀腐蚀, 而316L不锈钢均为轻微选择性腐蚀, Ni-P和Ni-Cu-P合金镀层均为均匀腐蚀.

关键词: Ni-Cu-P , Ni–P , J4 stainless steel , 316L stainless steel , liquid–solid two–phase flow , erosion and corrosion

J4不锈钢及化学镀Ni-P和Ni-Cu-P镀层在液-固两相流中的冲刷腐蚀行为

方信贤 , 白允强 , 王章忠

金属学报 doi:10.3724/SP.J.1037.2009.00499

用质量损失法系统研究了不同温度(25和50℃)和不同冲刷速率(0.63-1.88 m/s)下,J4不锈钢,Ni-P和Ni-Cu-P合金镀层,及对比材料316L不锈钢在液-固两相流(20%H_2SO_4+20 g/L Al_2O_3)中的冲刷腐蚀行为.结果表明:不锈钢和镀层的抗冲刷腐蚀性能由高到低依次为镀态Ni-Cu-P,镀态Ni-P,热处理态Ni-Cu-P,316L,J4.提高两相流介质温度均使它们的冲刷腐蚀速率增大.316L不锈钢在25℃液-固两相流介质中的冲刷腐蚀速率分别为镀态Ni-Cu-P,镀态Ni-P和热处理态Ni-Cu-P镀层的8.5倍,8倍和2.6倍以上,而在50℃下分别为392倍,80倍和14.8倍以上;J4不锈钢在25和50℃液-固两相流介质中的冲刷腐蚀速率分别为316L不锈钢的28倍和13倍以上.在25和50℃,J4不锈钢分别为选择性腐蚀和均匀腐蚀,而316L不锈钢均为轻微选择性腐蚀,Ni-P和Ni-Cu-P合金镀层均为均匀腐蚀.

关键词: Ni-Cu-P , Ni-P , J4不锈钢 , 316L不锈钢 , 液-固两相流 , 冲刷腐蚀

116HU聚酯亚胺无挥发浸渍树脂的性能及其在风电上的模拟结构试验

王君 , 邹家桂 , 陈政标 , 高建武 , 刘彦坤 , 张杰元 , 宋莎

绝缘材料

  为解决苯乙烯和甲基苯乙烯在VPI浸渍树脂应用于风力发电机中的不足,采用不饱和聚酯亚胺、引发剂和无挥发活性稀释剂研制出116HU聚酯亚胺无挥发浸渍树脂,并对其各项性能进行了研究。结果表明:116HU聚酯亚胺无挥发浸渍树脂的常规性能满足风力发电机的要求,其耐热等级可达H级。用该树脂浸渍的风电模拟线棒具有优异的介电性能、耐湿热交变和高低温循环冲击性能及耐盐雾性能等,能满足风力发电机在极端环境运行的要求。

关键词: 聚酯亚胺 , 无挥发 , VPI , 风力发电机 , 耐湿热 , 耐盐雾

J/Ψ衰变的Roper共振态结构的研究

平荣刚

原子核物理评论 doi:10.3969/j.issn.1007-4627.2004.02.026

通过J/Ψ→pp-,pN-*,N*N-*衰变,研究了Roper共振态的混杂态结构对衰变角分布和分支比的影响.计算结果表明,如果Roper共振态为纯混杂态,那么J/Ψ→pN-*,N*N-*的角分布几乎相等,而J/Ψ衰变到混杂态的衰变宽度还不到J/Ψ→pp-的1%,给出了Γ(J/Ψ→ N*p-)/Γ(J/Ψ→pp-)和Γ(J/Ψ→ N*N-*)/Γ(J/Ψ→pp-)随混合参数的变化关系,并讨论了在J/Ψ衰变中研究Roper混杂态结构的可能性.

关键词: Roper共振态结构 , 混杂态 , J

Spin waves in a four-sublattice Heisenberg ferrimagnet or ferromagnet with different exchange constants (J(ab)=J(cd)not equal J(bc)=J(da))

Physical Review B

The Hamiltonian for a four-sublattice Heisenberg ferrimagnet or ferromagnet with different exchange constants (J(ab) = J(cd) not equal J(bc) = J(da)) was established. An extended Bogoliubov transformation was developed by solving an equation group, consisting of 20 equations and 20 unknowns. The procedure for solving the equation group was carried out by introducing a simple way of reducing the numbers of the equations and the unknowns. The spin-wave spectra in the present system have been determined by performing the standard Holstein-Primakoff transformation and the Bogoliubov one. It has been found that the spin-wave spectra of the present system depend on the exchange constants and that the degeneracy of the spin-wave spectra remains. The results for a special case (J(ab) = J(bc)) i.e., an antiferromagnet are discussed briefly. The spin-wave spectra of the four-sublattice Heisenberg antiferromagnet are found to be degenerative also and they are linear in k for small k.

关键词: model

EFFECT OF SPECIMEN SIZE ON J_R RESISTANCE CURVE

H.P. Chen and Z.J. Deng (State Key Lab. for Mechanical Behavior of Materials , Xi'an Jiaotong University , Xi'an 710049 , China)

金属学报(英文版)

The effect of specimen thinkness on JR resistance curve has been investigated using low and middle strength steels. As the J dominance regime is reached, the initial J-integral values, J(i), are definite even if the elastic component Ji(e) and plastic component Ji(p)vary with the thinkness of specimen. The wider the specimen width, the larger the Ji(e)/Ji and the smaller the Ji(p)/Ji. The crack propagation resistance, dJR/da and dJp/da, decreases, while dJe/da increases linearly with increasing specimen thinness.Based on the above experimental results, an empirical formula dJ/da = α+β. B is given, which can be used to evaluate the safety of practical structural components.A modified J-integral is presented, upon which a new view is Put forward that the increase in crack growth resistance is induced mainly by the increase in the plastic J-integral component with the crack propagation,

关键词: : fracture mechanics , null , null , null

通过J/Ψ→N(N-)M衰变研究N*时的核子极点效应

沈彭年 , 梁伟红 , 邹冰松

原子核物理评论 doi:10.3969/j.issn.1007-4627.2004.02.009

研究了J/Ψ→ p(p-)π衰变过程中核子极点图的贡献,特别是由离壳效应带来的贡献.发现衰变宽度对形状因子是敏感的.在通过用J/Ψ→ p(p-)π衰变研究N*时,核子极点图作为背景道的贡献是非常重要的; 在通过J/Ψ→ p(p-)η和 p(p-)η研究N*时,核子极点图的贡献可忽略不计; 在通过J/Ψ→ p(p-)ω研究N*时,核子极点图有明显的贡献.

关键词: J/Ψ衰变 , 核子激发态

  • 首页
  • 上一页
  • 1
  • 2
  • 3
  • 4
  • 5
  • 下一页
  • 末页
  • 共1064页
  • 跳转 Go

出版年份

刊物分类

相关作者

相关热词