欢迎登录材料期刊网

材料期刊网

高级检索

  • 论文(16)
  • 图书()
  • 专利()
  • 新闻()

Numerical Simulation and Sensitivity Analysis of Parameters for Multistand Roll Forming of Channel Section With Outer Edge

ZENG Guo , LAI Xinmin , YU Zhongqi , LIN Zhongqin

钢铁研究学报(英文版)

Cold roll forming is a high production but complex metal forming process under the conditions of coupled effects with multifactor. A new booting finite element method (FEM) model using the updated Lagrangian (UL) method for multistand roll forming process is developed and validated. Compared with most of the literatures related to roll forming simulation, the new model can take the roll rotation into account and is well suited for simulating multistand roll forming. Based on the model, the process of a channel section with outer edge formed with twelve passes is simulated and the sensitivity analysis of parameters is conducted with orthogonal design combined FEM model. It is found that the multistand roll forming process can be efficiently analyzed by the new booting model, and sensitivity analysis shows that the yield strength plays an important role in controlling the quality of the products.

关键词: cold roll forming;multistand;roll forming;sensitivity;FEM model

表面包覆法合成的LiN0.8Co0.2O2材料的结构表征

刘欣艳 , 赵煜娟 , 夏定国

功能材料

LiNi0.8Co0.2O2是锂离子电池界公认的最有希望取代商业化正极材料LiCoO2的新型正极材料之一.本文所研究的复合正极材料LiNi0.8Co0.2O2是由细小的晶粒构成的球形颗粒,单一相,属于R3m空间群.对复合材料LiNi0.8Co0.2O2的Co-K和Ni-K的XANES分析可知,在600~850℃范围温度对于钴元素的影响不明显,而对于镍元素的影响比较显著,随着Ni-K边位置向高能量移动LiNi0.8Co0.2O2正极材料的放电容量升高.复合材料LiNi0.8Co0.2O2和LiNiO2的Ni-K边XANES相似,表明少量钴的引入对晶体结构的改变不是太多,但是峰的强度较高和峰的位置向高能量移动,表明钴Co对Ni的局域结构进行了调制.

关键词: LiNi0.8Co0.2O2 , XANES , 正极材料 , 局域结构

掺Mn硅酸锌薄膜中微量氧化锌对发光强度的影响

席俊华 , 季振国 , 刘坤 , 王超 , 杜鹃

无机材料学报 doi:10.3724/SP.J.1077.2006.01506

利用溶胶-凝胶法结合高温热处理在硅衬底上制备了掺Mn硅酸锌薄膜, 用XRD、SEM、UV-Vis吸收谱和PL谱测试了样品的结晶性能与光学性能, 并分析了热处理温度对掺Mn硅酸锌薄膜的结晶性能和光学性能的影响. 实验结果发现, ZnO的适量存在对掺Mn薄膜的发光有增强作用. 进一步的分析认为, 这一现象的机理可由G.G. Qin提出的量子约束-发光中心 (QCLC) 模型进行解释, ZnO中受激发的电子和空穴通过隧穿效应到达硅酸锌基体中复合发光, 从而增强发光强度.

关键词: 硅酸锌 , ZnO , photoluminescence , quantum confinement-luminescence center

Extended quantum confinement luminescence center model for photoluminescence from oxidized porous silicon and nanometer-Si-particle- or nanometer-Ge-particle-embedded silicon oxide films

Materials Research Bulletin

Through analysis of the latest experimental results reported in the literature and obtained in our laboratory, we have extended our previous quantum confinement/luminescence center model for the photoluminescence mechanism of porous Si and of nanometer-silicon-particle-embedded Si oxide films (G.G. Qin and Y.Q. Jia, Solid State Commun. 86, 559 (1993)). We consider that there are three main types of competitive photoexcitation/photoemission processes and that the process in which photoexcitation occurs in the nanometer silicon particles (NSPs) while photoemission occurs in the luminescence centers (LCs) in the SiOx layers very close to the NSPs is usually the major one. We discuss under what conditions the other two types of processes will dominate. We believe that the extended quantum confinement/luminescence center model is a physical model that is suitable for the photoluminescence from silicon oxide films embedded with NSPs or nanometer Ge particles (NGPs), as well as from oxidized porous Si. (C) 1999 Elsevier Science Ltd.

关键词: oxides;luminescence;defects;blue-light emission;visible luminescence;optical-properties;nanocrystals;mechanism;dependence;sio2-films;absorption;spectra;defects

Reply to "Comment on 'Low-temperature lattice excitation of icosahedral Al-Mn-Pd quasicrystals' "

Physical Review B

In response to the comment by Wang and Qin, we have rewritten our equation (22) following the coordinate system of Dina, et al. [J. Wuhan Univ. (Nature Science Edition) 3, 23 (1992)]. According to the thermodynamic stability condition and the experiment of Capitan et al., we have chosen the new parameters of the phason elastic constants. Based on this, we have recalculated the coefficients of the expressions on the vibrational denty of states and the specific heat of the icosahedral Al-Nin-Pd quasicrystal. Our results are still in agreement with the experimental data measured by Walti et al. [Phys. Rev. B 57, 10 504 (1998)]. It demonstrates that our method is useful for dealing with the low-temperature vibrational excitation of icosahedral quasicrystals.

关键词: quasi-crystals;diffuse-scattering

含取代茚基配体稀土金属有机化合物的合成、表征及催化性能

吴运军 , 张武 , 马怀柱

稀土 doi:10.3969/j.issn.1004-0277.2003.06.004

采用Schlenk技术,在干燥纯氩气保护下,用无水三氯化稀土LnCl3与2-苯基茚以1∶2的摩尔比在THF中反应,得到8种新配合物:(2-ph-Ind)2LnCl (A)[Ln=La(1), Pr(2), Nd(3), Sm(4), Gd(5), Dy(6), Yb(7), Y(8)].再用(A)和LiN(TMS)2在THF中反应,得到两种新的二(2-苯基茚)稀土有机配合物:(2-ph-Ind)2LnN(TMS)2 (B)[Ln=Y(1), Sm(2)].所有配合物都经元素分析、红外和质谱鉴定.配合物(B)在甲基丙烯酸甲酯(MMA)的聚合反应中显示出一定的活性.

关键词: 稀土合成 , 配合物 , 聚合 , 2-苯基茚

正极材料LiM0.9Ti0.1O2(M=Ni,Co)的合成及表征

贺慧 , 程璇 , 张颖 , 杨勇

功能材料

利用溶胶-凝胶预处理固相方法合成了锂离子电池正极材料LiM0.9Ti0.1O2(M=Ni,Co),通过XRD对合成的材料进行结构分析,并将其组装成电池进行了电化学测试,对两种材料LiN0.9Ti0.1和LiCo0.9Ti0.1进行了比较.结果发现,LiCo0.9Ti0.1O2的结构和性能要好于LiNi0.9Ti0.1O2,根据实验结果对其原因进行了初步的分析.

关键词: 锂离子电池 , 正极材料 , 电化学性能

掺Mn硅酸锌薄膜中微量氧化锌对发光强度的影响

席俊华 , 季振国 , 刘坤 , 王超 , 杜鹃

无机材料学报 doi:10.3321/j.issn:1000-324X.2006.06.038

利用溶胶-凝胶法结合高温热处理在硅衬底上制备了掺Mn硅酸锌薄膜,用XRD、SEM、UV-Vis吸收谱和PL谱测试了样品的结晶性能与光学性能,并分析了热处理温度对掺Mn硅酸锌薄膜的结晶性能和光学性能的影响.实验结果发现,ZnO的适量存在对掺Mn薄膜的发光有增强作用.进一步的分析认为,这一现象的机理可由G.G.Qin提出的量子约束-发光中心(QCLC)模型进行解释,ZnO中受激发的电子和空穴通过隧穿效应到达硅酸锌基体中复合发光,从而增强发光强度.

关键词: 硅酸锌 , 氧化锌 , 光致发光 , 量子约束-发光中心

天然气井油管悬挂器腐蚀失效分析

刘守平 , 周上祺 , 王佳眉 , 任勤

腐蚀学报(英文)

用金相显微镜、扫描电镜、X射线衍射仪和X射线能谱仪对天然气井油管悬挂器腐蚀失效进行了检测分析,并对天然气井油管悬挂器用35CrMo钢进行了盐雾试验,结果表明,天然气中的水和CO2是引起腐蚀的主要介质,腐蚀产物主要是FeCO3,高速天然气冲刷和钢中的非金属夹杂加剧了腐蚀的速度. CORROSION FAILURE ANALYSIS OF AN OIL TUBE USED IN NATURAL GAS WELL LIU Shou-ping,ZHOU Shang-qi,WANG Jia-mei,REN Qin Chongqing University A failed oil tube used in natural gas well was examined by optical microscope,scanning electron microscope ,X-ray diffractometer and X-ray spectrometer.Corrosion behavior of 35CrMo steel samples of the oil tube were investigated by means of salt spray tests in the laboratory.The results show that CO2 and H2O are primary factors in the corrosion of oil tube.The corrosion product is FeCO3,non-metallic inclusions in the steel and erosion of natural gas fluid played an important role in accelerating the corrosion. oil tube; natural gas well; 35CrMo steel; failure analysis; corrosion

关键词: 悬挂器 , null , null , null

  • 首页
  • 上一页
  • 1
  • 2
  • 下一页
  • 末页
  • 共2页
  • 跳转 Go

出版年份

刊物分类

相关作者

相关热词