ZHAO Jin-long
,
XI Yan
,
SHI Wen
,
LI Lin
钢铁研究学报(英文版)
Abstract: Microstructure evolution and mechanical properties of newly designed 01C-6Mn-05Si-1Al TRIP-aided steels under different annealing conditions and the effects of matrix microstructure before intercritical annealing on the final microstructure were studied by means of X-ray diffraction (XRD), scanning electron microcopy (SEM), dilatometric simulation, optical microstructure (OM) and tensile testing in this work. The experimental results indicate that the TRIP steel with Mn of 6% could form a considerable amount of retained austenite with good TRIP effect after a simple intercritical annealing treatment, and the matrix microstructure before intercritical annealing treatment can greatly affect the final microstructure. The original microstructure of the ferritic matrix steel was eliminated, while annealed martensite was remained from the martensite matrix steel under the same intercritical annealing conditions.
关键词:
Key words: high manganese TRIP steel
,
intercritical annealing
,
microstructure
,
mechanical properties
彭宁琦
,
唐广波
,
刘正东
,
吴秀月
金属学报
doi:10.3321/j.issn:0412-1961.2009.03.013
根据Aaronson提出的超组元模型,借助Ae3的实验数据,提出了修正的置换型元素Xi(Xi=Si,Mn,Ni,Co,Mo,Al,Cu,Cr)的Zener两参数,修正中考虑了合金元素间的交互作用.修正后的超组元模型的预测精度明显改善:Ae3计算值与实验值的标准差为10.8℃,与Thermo-Calc计算值的标准差为2.35℃;Ae1计算值与实验值的标准差为6.8℃.按照马氏体相变热力学的计算方法,采用经修正的参数计算了马氏体相变开始温度Ms,提高了Ms点的预测精度,计算值与实验值的标准差为25.3℃.
关键词:
相变
,
热力学
,
超组元模型
,
相变平衡温度
盛广
,
杨志刚
金属学报
根据Fe--C--Xi合金系的正平衡和准平衡热力学模型,推导了简便的奥氏体--铁素体相变驱动力计算解析式。根据公式, 代入合金原始成分和Ae3温度, 即可准确计算正平衡和准平衡模式下的奥氏体--铁素体相变驱动力。采用这一方法计算了Fe--C--Mn--Si--Ni--Cr--Mo--Cu八元系的正平衡和准平衡奥氏体--铁素体相变驱动力。