QIU Yiming ZHU Yaoxiao Institute of Metal Research , Academia Sinica , Shenyang , China Professor , Institute of Metal Research , Academia Sinica , Shenyang , China
金属学报(英文版)
An investigation was made on the possibility of using Ni-x phase diagrams to judge the sym- bol and degree of segregation of alloying element x in cast nickel-base superalloys.The pre- diction coincides with the experimental data.